| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Valox® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.64 g/cc | 1.64 g/cc | ASTM D792 |
| Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.0600 % | 0.0600 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.19 % | 0.19 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0018 - 0.0021 cm/cm @Thickness 3.20 mm |
0.0018 - 0.0021 in/in @Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0075 - 0.0094 cm/cm @Thickness 3.20 mm |
0.0075 - 0.0094 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 17.8 g/10 min @Load 5.00 kg, Temperature 250 °C |
17.8 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
| Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 250 °C |
12 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 110 MPa | 16000 psi | 5 mm/min; ISO 527 |
| 114 MPa | 16500 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 111 MPa | 16100 psi | 5 mm/min; ISO 527 |
| 116 MPa | 16800 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 2.1 % | 2.1 % | 5 mm/min; ISO 527 |
| 2.3 % | 2.3 % | Type I, 5 mm/min; ASTM D638 | |
| 2.9 % | 2.9 % | Flexural Strain, break, 2 mm/min; ISO 178 | |
| Elongation at Yield | 2.1 % | 2.1 % | 5 mm/min; ISO 527 |
| 2.2 % | 2.2 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 9.44 GPa | 1370 ksi | 1 mm/min; ISO 527 |
| 9.75 GPa | 1410 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 182 MPa | 26400 psi | 2 mm/min; ISO 178 |
| Flexural Yield Strength | 174 MPa | 25200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 183 MPa | 26500 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 6.74 GPa | 978 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 7.87 GPa | 1140 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
| 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1A |
| 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 13.0 J @Temperature 23.0 °C |
9.59 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 22.8 µm/m-°C @Temperature 23.0 - 80.0 °C |
12.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| 23.5 µm/m-°C @Temperature -40.0 - 95.0 °C |
13.1 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -40.0 - 95.0 °C |
63.3 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| 119 µm/m-°C @Temperature 23.0 - 80.0 °C |
66.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| Hot Ball Pressure Test | <= 75.0 °C | <= 167 °F | IEC 60695-10-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 221 °C @Thickness 6.40 mm |
430 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 188 °C | 370 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 197 °C @Thickness 3.20 mm |
387 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| 205 °C @Thickness 6.40 mm |
401 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 175 °C | 347 °F | Rate B/120; ISO 306 |
| 176 °C | 349 °F | Rate B/50; ASTM D1525 | |
| 176 °C | 349 °F | Rate B/50; ISO 306 | |
| Flammability, UL94 | V-0 @Thickness 0.800 mm |
V-0 @Thickness 0.0315 in |
UL 94 by SABIC-IP |