Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature of 245 °C and HDT of 235 °C, the resin extends the thermal capability range available in other sulfone polymers. The resin is completely amorphous and fully thermoplastic allowing easy melt fabrication by means of injection molding and other thermoplastic processing techniques. Along with its high thermal performance capabilities, HTS-2401 resin also boasts a long list of high performance attributes which include excellent hydrolytic stability, resistance to acids and bases and inherently flame retardant performance to mention a few. The ease of melt fabrication, coupled with the completely amorphous character assures tight dimensional control during injection molding of precision parts and components. The versatile performance profile of HTS-2401 makes it a good candidate for metal replacement or the replacement of difficult-to-process thermoplastics in a wide range of engineering applications. In its natural state, Supradel HTS-2401 resin is transparent with an amber/brown color.Information provided by Solvay Advanced Polymers
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 0.40 %
0.40 %
At 24 hours; ASTM D570
Water Absorption at Saturation 1.4 %
1.4 %
ASTM D570
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Melt Flow 27 g/10 min

@Load 5.00 kg,
Temperature 400 °C
27 g/10 min

@Load 11.0 lb,
Temperature 752 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Elongation at Yield 7.5 %
7.5 %
ASTM D638
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Flexural Strength 94.5 MPa
13700 psi
ASTM D790
Flexural Modulus 2.32 GPa
336 ksi
ASTM D790
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
Annealed 0.125 inch thick specimen; ASTM D648
Glass Transition Temp, Tg 245 °C
473 °F
Optical Properties Metric English Comments
Refractive Index 1.66
1.66
ASTM D542
Processing Properties Metric English Comments
Melt Temperature 390 - 410 °C
734 - 770 °F
Stock Temperature
Mold Temperature >= 160 °C
>= 320 °F
170 - 190 °C
338 - 374 °F
Long flow or thin wall parts or for low residual stress
Drying Temperature 150 °C
302 °F
2.5 hours for injection molding
170 °C
338 °F
> 4 hours hopper drying with desiccated air inlet for extrusion
Users viewing this material also viewed the following: