| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled |
| Manufacturer | Addiplast |
| Trade Name | Addinyl |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Addiplast Addinyl A2 V15 Nylon 66, 15% Glass Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 80 | 80 | Conditioned; ISO 868 |
| 85 | 85 | ISO 868 | |
| Tensile Strength at Break | 90.0 MPa | 13100 psi | Conditioned; ISO R 527 |
| 130 MPa | 18900 psi | ISO R 527 | |
| Elongation at Yield | 5.0 % | 5.0 % | ISO R 527 |
| 13 % | 13 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 3.50 GPa | 508 ksi | Conditioned; ISO 178 |
| 6.00 GPa | 870 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180/1A |
| 5.50 kJ/m² | 2.62 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/IeU |
| 5.50 J/cm² | 26.2 ft-lb/in² | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179/IeA |
| 0.500 J/cm² | 2.38 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 35.0 µm/m-°C | 19.4 µin/in-°F | ASTM E831 |
| Melting Point | 260 °C | 500 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | ISO 75-2/AF |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | Conditioned; CEI 60243-1 |
| 33.0 kV/mm | 838 kV/in | CEI 60243-1 | |
| Comparative Tracking Index | 600 V | 600 V | CEI 60112/Solution A |