| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | Unitika |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Unitika A1030BRL PA6, Dry.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Water Absorption | 1.8 % @Time 86400 sec |
1.8 % @Time 24.0 hour |
ISO 62 |
| Moisture Absorption at Equilibrium | 2.8 % | 2.8 % | 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.010 cm/cm @Thickness 3.20 mm |
0.010 in/in @Thickness 0.126 in |
|
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm @Thickness 3.20 mm |
0.013 in/in @Thickness 0.126 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 112 | 112 | ISO 2039 |
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | ISO 527-1/-2 |
| Elongation at Break | 45 % | 45 % | ISO 527-1/-2 |
| Elongation at Yield | 5.0 % | 5.0 % | ISO 527-1/-2 |
| Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
| Flexural Strength | 99.0 MPa | 14400 psi | ISO 178 |
| Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
| Charpy Impact Unnotched | NB | NB | ISO 179-1 |
| Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 96.0 µm/m-°C | 53.3 µin/in-°F | ISO 11359-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO 75-1/-2 |
| Flammability, UL94 | V-2 @Thickness 0.840 mm |
V-2 @Thickness 0.0331 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 3.00e+13 ohm-cm | 3.00e+13 ohm-cm | IEC 60093 |
| Dielectric Constant | 3.4 @Frequency 1.00e+6 Hz |
3.4 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Dielectric Strength | 37.0 kV/mm @Thickness 1.00 mm |
940 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
| Dissipation Factor | 0.020 @Frequency 1.00e+6 Hz |
0.020 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | >= 600 V | >= 600 V | IEC 60112 |