Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0035 - 0.0045 cm/cm | 0.0035 - 0.0045 in/in | |
Ovation Polymers RIGITRON 20415 GF PBT, 15% Glass Reinforced PBT - Glass reinforced (15 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared acco.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0045 cm/cm | 0.0015 - 0.0045 in/in | Injection and Compression; ISO 2577 |
Raschig Group 2567 AMC Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and .. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | Injection and Compression; ISO 2577 |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0045 cm/cm | 0.0020 - 0.0045 in/in | Injection; ISO 2577 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0045 cm/cm | 0.0015 - 0.0045 in/in | ISO 2577 |
Raschig Group 5553 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0045 cm/cm | 0.0015 - 0.0045 in/in | Injection; ISO 2577 |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0045 cm/cm | 0.0015 - 0.0045 in/in | Injection; ISO 2577 |
Raschig Group 5563 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0045 cm/cm | 0.0020 - 0.0045 in/in | Injection; ISO 2577 |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | ISO 2577 |
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | (longitudinal); ISO 2577 |
Raschig Group 3572 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | ASTM D955 |
PlastxWorld CEVIAN® B6524 20% GF PBT/ABS Alloy Glass fiber and mineral filled, low warpage and flame retarded PBT/ABS.Information provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.0035 - 0.0045 cm/cm | 0.0035 - 0.0045 in/in | ISO 2577 |
Polyram PlusTek PA320G3 Nylon 6.6 for Injection Molding, 15% Glass Fiber Reinforced, Flame Retardant 15% Glass fiber reinforced flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0045 cm/cm | 0.0020 - 0.0045 in/in | ISO 2577 |
Polyram Polytron P60B08-S Polypropylene, 60% Long Glass Fiber Polytron P60B08-S (Single strand) is a chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0045 cm/cm | 0.0030 - 0.0045 in/in | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
Bulk Molding Compounds BMC 610 - SP Mineral Filled, Glass Reinforced Polyester Compound, with UV Stabilizer BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
Bulk Molding Compounds BMC 610 Mineral filled, glass-fiber-reinforced polyester compound BMC 610 molding compound is a mineral filled, glass fiber reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
Bulk Molding Compounds BMC 610 Mineral Filled, Glass Reinforced Polyester Compound BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYabs F20 GF17 ABS, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | With Flow; ISO 2577 |
Polykemi AB POLYabs F20 GF17 ABS, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0020 - 0.0045 cm/cm | 0.0020 - 0.0045 in/in | Injection; ISO 2577 |
Raschig Group 5557 DAP
(discontinued **) Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h.. |
|||
Linear Mold Shrinkage | 0.0035 - 0.0045 cm/cm | 0.0035 - 0.0045 in/in | |
Polyram PlusTek RA320G3 Nylon 6.6, 15% Glass Fiber, Flame Retardant 15% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |