Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
(DAM); ISO 1183
Water Absorption 6.3 %
6.3 %
DAM; Sim. to ISO 62
Moisture Absorption at Equilibrium 1.9 %
1.9 %
Humidity Absorption (DAM); Sim. to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527-1/-2
Elongation at Break 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 6.50 GPa
943 ksi
ISO 527-1/-2
Charpy Impact Unnotched 7.00 J/cm²

@Temperature -30.0 °C
33.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
11.0 J/cm²

@Temperature 23.0 °C
52.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 9200 MPa
1.33e+6 psi
ISO 899-1
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min (DAM); ISO 11357-1/-3
UL RTI, Electrical 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL746B
140 °C

@Thickness 0.750 mm
284 °F

@Thickness 0.0295 in
UL746B
UL RTI, Mechanical with Impact 120 °C

@Thickness 0.750 mm
248 °F

@Thickness 0.0295 in
UL746B
125 °C

@Thickness 1.50 mm
257 °F

@Thickness 0.0591 in
UL746B
UL RTI, Mechanical without Impact 140 °C

@Thickness 0.750 mm
284 °F

@Thickness 0.0295 in
UL746B
150 °C

@Thickness 1.50 mm
302 °F

@Thickness 0.0591 in
UL746B
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 5.0

@Frequency 1e+6 Hz
5.0

@Frequency 1e+6 Hz
IEC 60250
20

@Frequency 100 Hz
20

@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1
Dissipation Factor 0.12

@Frequency 1e+6 Hz
0.12

@Frequency 1e+6 Hz
IEC 60250
0.30

@Frequency 100 Hz
0.30

@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 400 - 599 V
400 - 599 V
PLC 1; UL 746A
500 V
500 V
IEC 60112
Descriptive Properties Value Comments
Heat stabilized or stable to heat Yes
Injection molding Yes