Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Montell 1900LCM UHMW Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer LyondellBasell
Trade Name Montell
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Montell 1900LCM UHMW Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferApplications: wear surfaces in pulp and paper process, material handling and packaging equipment, food and beverage processing systems, impact and abrasion resistant parts for mining and solid waste handling, marine fendering, battery separatorsMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: 1900LCM ultrahigh molecular wight polyethylene resin has an average molecular weight range between 3 and 5 million. This polymer is for use in compression moldind, solution and ram extrusion processes. It is supplied in a fine powder form with calcium stearate added as a dry flow processing aid. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All indgredients meet the chemical regristration requirments of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Apparent Bulk Density 0.470 - 0.470 g/cc
0.0170 - 0.0170 lb/in³
ASTM D792
Viscosity Test 2300 cm³/g
2300 cm³/g
Intrinsic; ASTM D4020
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 0.750 GPa
109 ksi
1% secant at 0.05 in/min; ASTM D790B
Izod Impact, Notched NB
NB
ASTM D256
Abrasion 8.5
8.5
% Abrasion Index; Montell P116 Test