Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Xenoy® X4850 PBT+PC

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Xenoy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Xenoy® X4850 PBT+PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional stability. The X4850 could be positioned for body panels, safety equipment,housings, doorhandles, spring-loaded applications, medical device enclosures, outdoor sports equipment.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Moisture Absorption 0.140 %
0.140 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.42 %
0.42 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm

@Thickness 3.20 mm
0.0070 - 0.0090 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 266 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
Melt Index of Compound 4.0 g/10 min

@Load 5.00 kg,
Temperature 265 °C
4.0 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
50 mm/min; ISO 527
50.0 MPa
7250 psi
5 mm/min; ISO 527
55.0 MPa
7980 psi
Type I, 50 mm/min; ASTM D638
60.0 MPa
8700 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 58.0 MPa
8410 psi
Type I, 5 mm/min; ASTM D638
58.0 MPa
8410 psi
5 mm/min; ISO 527
63.0 MPa
9140 psi
50 mm/min; ISO 527
65.0 MPa
9430 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 30 %
30 %
50 mm/min; ISO 527
80 %
80 %
5 mm/min; ISO 527
130 %
130 %
Type I, 50 mm/min; ASTM D638
140 %
140 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 3.4 %
3.4 %
5 mm/min; ISO 527
3.5 %
3.5 %
50 mm/min; ISO 527
3.7 %
3.7 %
Type I, 50 mm/min; ASTM D638
3.8 %
3.8 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 3.85 GPa
558 ksi
1 mm/min; ISO 527
4.00 GPa
580 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 94.0 MPa
13600 psi
2 mm/min; ISO 178
99.0 MPa
14400 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.50 GPa
508 ksi
2 mm/min; ISO 178
3.70 GPa
537 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.80 J/cm
3.37 ft-lb/in
ASTM D256
1.00 J/cm

@Temperature -30.0 °C
1.87 ft-lb/in

@Temperature -22.0 °F
ASTM D256
1.20 J/cm

@Temperature 0.000 °C
2.25 ft-lb/in

@Temperature 32.0 °F
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1A
7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
11.0 kJ/m²

@Temperature 0.000 °C
5.23 ft-lb/in²

@Temperature 32.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NB
NB
Edgew 80*10*4 sp=62mm; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
60.0 J

@Temperature -20.0 °C
44.3 ft-lb

@Temperature -4.00 °F
ASTM D3763
Impact Test 100 J
73.8 ft-lb
Multiaxial Impact; ISO 6603
Taber Abrasion, mg/1000 Cycles 30
30
CS-17, 1 kg; SABIC Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
63.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
35.0 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
81.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
45.0 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
125 °C

@Thickness 3.20 mm
257 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
210 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
101 °C

@Thickness 3.20 mm
214 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 133 °C
271 °F
Rate B/50; ISO 306
134 °C
273 °F
Rate B/50; ASTM D1525
135 °C
275 °F
Rate B/120; ISO 306
Users viewing this material also viewed the following: