| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | DAM; ASTM D792 |
| Water Absorption | 3.0 % @Temperature 23.0 °C |
3.0 % @Temperature 73.4 °F |
Equilibrium 50%RH; DAM; ASTM D570 |
| Linear Mold Shrinkage | 0.012 cm/cm @Thickness 3.20 mm |
0.012 in/in @Thickness 0.126 in |
Flow; DAM |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 50.0 MPa @Temperature 23.0 °C |
7250 psi @Temperature 73.4 °F |
50%RH; ASTM D638 |
| 80.0 MPa @Temperature 23.0 °C |
11600 psi @Temperature 73.4 °F |
DAM; ASTM D638 | |
| Tensile Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
50%RH; ASTM D638 |
| 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
DAM; ASTM D638 | |
| Izod Impact, Notched | 0.480 J/cm @Temperature -40.0 °C |
0.899 ft-lb/in @Temperature -40.0 °F |
DAM; ASTM D256 |
| 1.33 J/cm @Temperature 23.0 °C |
2.49 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 | |
| 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | DAM; ASTM D3418 |
| 220 °C | 428 °F | 10°C/min; DAM; ISO 11357-1/-3 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DAM; ISO 75-1/-2 |
| 160 °C | 320 °F | DAM; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | DAM; ASTM D648 |
| 65.0 °C | 149 °F | DAM; ISO 75-1/-2 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 230 - 240 °C | 446 - 464 °F | DAM; Extrusion |
| 235 °C | 455 °F | DAM; Optimum; Extrusion | |
| 270 °C | 518 °F | DAM; Optimum; Injection Molding | |
| 260 - 280 °C | 500 - 536 °F | DAM; Injection Molding | |
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | DAM; Injection Molding |
| 70.0 °C | 158 °F | DAM; optimum; Injection Molding | |
| Drying Temperature | 80.0 °C | 176 °F | DAM; Injection Molding |
| 80.0 °C | 176 °F | DAM; Extrusion | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM; Injection Molding |
| 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Extrusion | |
| Moisture Content | <= 0.050 % | <= 0.050 % | DAM; Injection Molding |
| <= 0.050 % | <= 0.050 % | DAM; Extrusion |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | DAM |
| Drying Recommended | Yes, if moisture content of resin exceeds recommended level | DAM |
| Features | Chemical Resistance, Good | DAM |
| Fuel Resistant | DAM | |
| Grease Resistant | DAM | |
| Oil Resistant | DAM | |
| Forms | Pellets | DAM |
| Generic | Nylon 6 | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA6< | ISO 11469; DAM |
| Processing Method | Extrusion | DAM |
| Injection Molding | DAM | |
| Product Category | Extrusion Resins | DAM |
| Unreinforced Resins | DAM | |
| Resin Identification | PA6 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |
| Uses | Appliance Components | DAM |
| Automotive Applications | DAM | |
| Electrical/Electronic Applications | DAM | |
| Industrial Applications | DAM |