| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® FN727 BK230A Nylon 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.02 g/cc | 0.0368 lb/in³ | DAM; ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0080 cm/cm @Thickness 2.00 mm |
0.0080 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 28.0 MPa @Temperature 23.0 °C |
4060 psi @Temperature 73.4 °F |
DAM; ISO 527 |
| Elongation at Break | >= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
DAM; nominal; ISO 527 |
| 130 % @Temperature 23.0 °C |
130 % @Temperature 73.4 °F |
DAM; nominal; ISO 527 | |
| 160 % @Temperature 23.0 °C |
160 % @Temperature 73.4 °F |
DAM; ISO 527 | |
| Tensile Modulus | 0.900 GPa @Temperature 23.0 °C |
131 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
| Flexural Modulus | 0.850 GPa @Temperature 23.0 °C |
123 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
| Izod Impact, Notched (ISO) | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
DAM; ISO 180/1A |
| Charpy Impact, Notched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 221 °C | 430 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 58.0 °C | 136 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 48.0 °C | 118 °F | DAM; ISO 75-1/-2 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 230 - 240 °C | 446 - 464 °F | DAM; Extrusion |
| 235 °C | 455 °F | DAM; Optimum; Extrusion | |
| 260 °C | 500 °F | DAM; Optimum; Injection Molding | |
| 250 - 280 °C | 482 - 536 °F | DAM; Injection Molding | |
| Mold Temperature | 60.0 °C | 140 °F | DAM; optimum; Injection Molding |
| 40.0 - 80.0 °C | 104 - 176 °F | DAM; Injection Molding | |
| Drying Temperature | 80.0 °C | 176 °F | DAM; Extrusion |
| 80.0 °C | 176 °F | DAM; Injection Molding | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM; Injection Molding |
| 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Extrusion | |
| Moisture Content | <= 0.050 % | <= 0.050 % | DAM; Extrusion |
| <= 0.050 % | <= 0.050 % | DAM; Injection Molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Black Color | DAM |
| Features | Chemical Resistance, Good | DAM |
| Chemical Resistance, Good | DAM | |
| Flexibility, Good | DAM | |
| Flexibility, Good | DAM | |
| Heat Aging Resistance, Good | DAM | |
| Heat Aging Resistance, Good | DAM | |
| Impact Modified | DAM | |
| Impact Modified | DAM | |
| Forms | Pellets | DAM |
| Generic | Nylon 6 | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA6-F< | ISO 11469; DAM |
| Processing Method | Extrusion | DAM |
| Product Category | Extrusion Resins | DAM |
| Toughened Resins | DAM | |
| Unreinforced Resins | DAM | |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA6-F | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |
| Uses | Cable Jacketing | DAM |
| Cable Jacketing | DAM | |
| Hose | DAM | |
| Hose | DAM | |
| Tubing | DAM | |
| Tubing | DAM |