| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 80 | 80 | Conditioned; ISO 868 |
| 85 | 85 | ISO 868 | |
| Tensile Strength at Break | 135 MPa | 19600 psi | Conditioned; ISO R 527 |
| 180 MPa | 26100 psi | ISO R 527 | |
| Elongation at Yield | 3.0 % | 3.0 % | ISO R 527 |
| 5.0 % | 5.0 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 5.80 GPa | 841 ksi | Conditioned; ISO 178 |
| 8.20 GPa | 1190 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | ISO 180/1A |
| 16.0 kJ/m² | 7.61 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/IeU |
| 6.50 J/cm² | 30.9 ft-lb/in² | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/IeA |
| 1.50 J/cm² | 7.14 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM E831 |
| Melting Point | 260 °C | 500 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75-2/AF |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | Conditioned; CEI 60243-1 |
| 35.0 kV/mm | 889 kV/in | CEI 60243-1 | |
| Comparative Tracking Index | 600 V | 600 V | CEI 60112/Solution A |