| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade |
| Manufacturer | Addiplast |
| Trade Name | Addinyl |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Addiplast Addinyl PMD 20164 Nylon 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 80 | 80 | Conditioned; ISO 868 |
| 82 | 82 | ISO 868 | |
| Tensile Strength at Break | 90.0 MPa | 13100 psi | Conditioned; ISO R 527 |
| 130 MPa | 18900 psi | ISO R 527 | |
| Elongation at Yield | 4.0 % | 4.0 % | ISO R 527 |
| 6.0 % | 6.0 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 5.00 GPa | 725 ksi | Conditioned; ISO 178 |
| 8.00 GPa | 1160 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180/1A |
| 25.0 kJ/m² | 11.9 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/IeU |
| 9.00 J/cm² | 42.8 ft-lb/in² | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/IeA |
| 2.50 J/cm² | 11.9 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | ISO 75-2/AF |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Comparative Tracking Index | >= 600 V | >= 600 V | CEI 60112/Solution A |