Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating

Category Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Aremco
Trade Name Quartz-Coat™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadium lighting and quartz vessels for the semiconductor industry. Standard viscosity is 200–400 cP; a higher viscosity coating, 845-HV, in the range of 500–800 cP is available upon request.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
Solids Content 22.9 %
22.9 %
by volume
50.1 %
50.1 %
by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Viscosity 200 - 400 cP
200 - 400 cP
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
82.3 microns
3.24 mil
estimated wet film thickness
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1090 °C
2000 °F
Continuous
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Cure Time 5.00 min

@Temperature 482 °C
0.0833 hour

@Temperature 900 °F
Step 2
10.0 min

@Temperature 93.3 °C
0.167 hour

@Temperature 200 °F
Step 1, preceeded by >10 min. air set
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Brown-Black
Cured
Dry Film Coverage ft2/gal 495
at 1 mil
Thinner 845-T