| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.34 g/cc | 0.0484 lb/in³ | DAM; ISO 1183 |
| Filler Content | 30 % | 30 % | DAM |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 110 MPa @Temperature 23.0 °C |
16000 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Elongation at Break | 3.0 % @Temperature 23.0 °C |
3.0 % @Temperature 73.4 °F |
DAM; ISO 527 |
| 6.0 % @Temperature 23.0 °C |
6.0 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| Tensile Modulus | 5.60 GPa @Temperature 23.0 °C |
812 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 9.40 GPa @Temperature 23.0 °C |
1360 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Flexural Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
| 9.00 GPa @Temperature 23.0 °C |
1310 ksi @Temperature 73.4 °F |
DAM; ISO 178 | |
| Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A |
| 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A | |
| 17.0 kJ/m² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A | |
| 22.0 kJ/m² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1U |
| 75.0 kJ/m² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1U | |
| Charpy Impact Unnotched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
| 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU | |
| Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
| 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA | |
| 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA | |
| 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
| 500 µm/m-°C @Temperature 23.0 - 55.0 °C |
278 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| 500 µm/m-°C @Temperature 55.0 - 160 °C |
278 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
| 107 µm/m-°C @Temperature 23.0 - 55.0 °C |
59.4 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| 110 µm/m-°C @Temperature 55.0 - 160 °C |
61.1 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| Melting Point | 221 °C | 430 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 206 °C | 403 °F | DAM; ISO 75-1/-2 |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; UL94 |
| HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; IEC 60695-11-10 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | DAM |
| 270 °C | 518 °F | DAM; Optimum | |
| Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | DAM |
| 80.0 °C | 176 °F | DAM; optimum | |
| Drying Temperature | 80.0 °C | 176 °F | DAM |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
| Moisture Content | <= 0.20 % | <= 0.20 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Impact Modifier | DAM |
| Appearance | Black Color | DAM |
| Drying Recommended | Yes, if moisture content of resin exceeds recommended level | DAM |
| Features | Chemical Resistance, Good | DAM |
| Fatigue Resistant | DAM | |
| Fuel Resistant | DAM | |
| Grease Resistant | DAM | |
| Impact Modified | DAM | |
| Impact Resistance, Good | DAM | |
| Oil Resistant | DAM | |
| Toughness, Good | DAM | |
| Filler | Glass fiber reinforcement | DAM |
| Forms | Pellets | DAM |
| Generic | Nylon 6 | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA6-IGF30< | ISO 11469; DAM |
| Polymer Family | Polyamide | DAM |
| Polymer Type | PA6 | DAM |
| Processing Method | Injection Molding | DAM |
| Product Category | Glass Reinforced Resins | DAM |
| Toughened Resins | DAM | |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA6-IGF30 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |
| Uses | Appliance Components | DAM |
| Automotive Applications | DAM | |
| Electrical/Electronic Applications | DAM | |
| High Gloss Applications | DAM | |
| Industrial Applications | DAM |