| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | DAM; ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0068 cm/cm @Thickness 2.00 mm |
0.0068 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.010 cm/cm @Thickness 2.00 mm |
0.010 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 65.0 MPa @Temperature 23.0 °C |
9430 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 93.0 MPa @Temperature 23.0 °C |
13500 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Elongation at Break | 14 % @Temperature 23.0 °C |
14 % @Temperature 73.4 °F |
DAM; ISO 527 |
| 18 % @Temperature 23.0 °C |
18 % @Temperature 73.4 °F |
DAM; 50mm/min; ISO 527 | |
| 40 % @Temperature 23.0 °C |
40 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| 57 % @Temperature 23.0 °C |
57 % @Temperature 73.4 °F |
50%RH; 50mm/min; ISO 527 | |
| Elongation at Yield | 4.7 % @Temperature 23.0 °C |
4.7 % @Temperature 73.4 °F |
DAM; ISO 527 |
| 19 % @Temperature 23.0 °C |
19 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| Tensile Modulus | 1.94 GPa @Temperature 23.0 °C |
281 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 3.40 GPa @Temperature 23.0 °C |
493 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
| 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | DAM; ISO 75-1/-2 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 290 °C | 554 °F | DAM; optimum |
| 280 - 300 °C | 536 - 572 °F | DAM | |
| Mold Temperature | 70.0 °C | 158 °F | DAM; Optimum |
| 50.0 - 90.0 °C | 122 - 194 °F | DAM | |
| Drying Temperature | 80.0 °C | 176 °F | DAM |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM; Dehumidified Dryer |
| Moisture Content | <= 0.20 % | <= 0.20 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | |
| Forms | Pellets | |
| Generic | PA66 | |
| Material Status | Preliminary Data | |
| Part Marking Code | >PA66< | ISO 11469 |
| Processing Method | Injection Molding | |
| Product Category | Extrusion Resins | |
| Region Available - Global | Yes | |
| Resin Identification | PA66 | ISO 1043 |
| RoHS Compliance | Contact Manufacturer | |
| Uses | Food Applications, Non-specific |