| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled , Polybutylene Terephthalate (PBT), Heat Resistant |
| Manufacturer | Eurotec |
| Trade Name | Tecodur® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Eurotec® Tecodur® PB70 GR30 NL XA70 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.200 % @Temperature 23.0 °C |
0.200 % @Temperature 73.4 °F |
50% RH; ISO 960 |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | Eurotec |
| Linear Mold Shrinkage, Transverse | 0.010 cm/cm | 0.010 in/in | Eurotec |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 130 MPa | 18900 psi | ISO 527 |
| Elongation at Break | 2.0 % | 2.0 % | ISO 527 |
| Tensile Modulus | 11.0 GPa | 1600 ksi | ISO 527 |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
| 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
| 60.0 kJ/m² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 225 °C | 437 °F | [10 K/min], ISO 11357 |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 205 °C | 401 °F | ISO 75 |
| Vicat Softening Point | 210 °C @Load 5.10 kg |
410 °F @Load 11.2 lb |
ISO 306 |
| Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
|
| Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI; IEC 60695 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
| Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 230 - 260 °C | 446 - 500 °F | |
| Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
| Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | |
| Drying Temperature | 120 °C | 248 °F | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
| Moisture Content | <= 0.080 % | <= 0.080 % | ISO 960 |
| Hold Pressure | 40.0 - 80.0 MPa | 5800 - 11600 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Injection Speed | Medium - Fast |