| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | Nilit (formerly Frisetta Polymer) |
| Trade Name | FRIANYL |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Nilit FRIANYL B63 KLZ Nylon 6 for injection molding.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Water Absorption | 1.5 - 2.8 % | 1.5 - 2.8 % | ISO 62 |
| Water Absorption at Saturation | 7.0 - 9.0 % | 7.0 - 9.0 % | ISO 62 |
| Viscosity Measurement | 145 | 145 | Viscosity index; ISO 307 |
| Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | FRISETTA Test Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
| Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527 |
| Elongation at Break | 10 % | 10 % | ISO 527 |
| Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
| Flexural Strength | 90.0 MPa | 13100 psi | ISO 178 |
| Flexural Modulus | 2.70 GPa | 392 ksi | ISO 178 |
| Charpy Impact Unnotched | NB | NB | DIN 53453 |
| NB @Temperature -40.0 °C |
NB @Temperature -40.0 °F |
DIN 53453 | |
| Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | DIN 53453 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 221 °C | 430 °F | ISO 3146 DSC |
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous; FRISETTA Test Method |
| Deflection Temperature at 0.46 MPa (66 psi) | 170 °C | 338 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | ISO 75 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 93 |
| Dissipation Factor | 0.020 @Frequency 1e+6 Hz |
0.020 @Frequency 1e+6 Hz |
IEC 250 |
| Comparative Tracking Index | 600 V | 600 V | CTI 100; IEC 112 |
| 600 V | 600 V | CTI-M 100; IEC 112 |