| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Bergamid™ A700 BK VN4255 LS Polyamide 66 (Nylon 66).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ±0.02 g/cm³; DIN 53479 |
| Water Absorption | 2.8 % | 2.8 % | 23C/50RH; ISO 62 |
| Water Absorption at Saturation | 8.5 % | 8.5 % | ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 80.0 MPa <br>@Temperature 23.0 °C |
11600 psi <br>@Temperature 73.4 °F |
dry as moulded; ISO 527-2/50 |
| Elongation at Yield | 4.5 % <br>@Temperature 23.0 °C |
4.5 % <br>@Temperature 73.4 °F |
dry as moulded; ISO 527-2/50 |
| Tensile Modulus | 3.20 GPa <br>@Temperature 23.0 °C |
464 ksi <br>@Temperature 73.4 °F |
dry as moulded; ISO 527-2/1 |
| Charpy Impact Unnotched | NB <br>@Temperature 23.0 °C |
NB <br>@Temperature 73.4 °F |
ISO 179/1eU |
| NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 0.400 J/cm² <br>@Temperature -30.0 °C |
1.90 ft-lb/in² <br>@Temperature -22.0 °F |
ISO 179/1eA |
| 0.600 J/cm² <br>@Temperature 23.0 °C |
2.86 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 261 °C | 502 °F | ISO 3146 |
| Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous (GTP 50% Tensile); IEC 60216 |
| 200 °C | 392 °F | Short Time; IEC 60216 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | Unannealed; ISO 75-2/B |
| Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Unannealed; ISO 75-2/A |
| Flammability, UL94 | V-2 <br>@Thickness 0.700 mm |
V-2 <br>@Thickness 0.0276 in |
ALL; Internal Method |
| Glow Wire Test | 675 °C <br>@Thickness 0.800 - 3.00 mm |
1250 °F <br>@Thickness 0.0315 - 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
| >= 800 °C <br>@Thickness 0.800 - 3.00 mm |
>= 1470 °F <br>@Thickness 0.0315 - 0.118 in |
Flammability Index; IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
| Dielectric Constant | 5.0 <br>@Frequency 1.00e+6 Hz |
5.0 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.20 <br>@Frequency 1.00e+6 Hz |
0.20 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 600 V | 600 V | Solution A; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Forms | Pellets | |
| Generic Material | Nylon 66 | |
| Generic Name | Polyamide 66 (Nylon 66) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| RoHS Compliance | RoHS Compliant |