| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.21 g/cc | 1.21 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 70 | 70 | ASTM D785 |
| Hardness, Rockwell R | 118 | 118 | ASTM D785 |
| Tensile Strength at Break | 60.0 MPa | 8700 psi | ASTM D638 |
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
| Elongation at Break | 90 % | 90 % | ASTM D638 |
| Elongation at Yield | 7.0 % | 7.0 % | ASTM D638 |
| Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
| Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
| Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 135 °C | 275 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
| Vicat Softening Point | 146 °C | 295 °F | 120°C/h, 50 N; ASTM D1525 |
| UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
| 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 | |
| UL RTI, Mechanical with Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
| 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 | |
| UL RTI, Mechanical without Impact | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746 |
| 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 | |
| Flammability, UL94 | V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
|
| V-0 @Thickness 3.00 mm |
V-0 @Thickness 0.118 in |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 1.0 % | 1.0 % | ASTM D1003 |
| UV Transmittance | 85 % | 85 % | ASTM D1003 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Dielectric Strength | 25.2 kV/mm | 640 kV/in | ASTM D149 |
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746 |
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
| 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 | |
| High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 1.50 mm |
15 - 30 arcs @Thickness 0.0591 in |
UL 746 |
| 30 - 60 arcs @Thickness 3.00 mm |
30 - 60 arcs @Thickness 0.118 in |
UL 746 | |
| High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
| Melt Temperature | 288 - 316 °C | 550 - 600 °F | |
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Vent | 0.0005 |