| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics NORYL PX1005X PPE+HIPS (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.0600 % | 0.0600 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.30 % | 0.30 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; SABIC Method |
| Melt Index of Compound | 6.0 g/10 min @Load 1.20 kg, Temperature 280 °C |
6.0 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, H358/30 | 90.0 MPa | 13100 psi | ISO 2039-1 |
| Tensile Strength at Break | 35.0 MPa | 5080 psi | 50 mm/min; ISO 527 |
| Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
| Elongation at Break | 15 % | 15 % | 50 mm/min; ISO 527 |
| Elongation at Yield | 3.0 % | 3.0 % | 50 mm/min; ISO 527 |
| Tensile Modulus | 2.10 GPa | 305 ksi | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 70.0 MPa | 10200 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 2.10 GPa | 305 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | 80*10*4; ISO 180/1A |
| 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA | |
| Taber Abrasion, mg/1000 Cycles | 80 | 80 | CS-17, 1 kg; SABIC Method |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
| CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| Vicat Softening Point | 95.0 °C | 203 °F | Rate B/120; ISO 306 |
| 105 °C | 221 °F | Rate A/50; ISO 306 | |
| Flammability, UL94 | HB @Thickness 1.00 mm |
HB @Thickness 0.0394 in |
UL 94 |
| V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
UL 94 | |
| 5VA @Thickness 3.00 mm |
5VA @Thickness 0.118 in |
UL 94 | |
| Oxygen Index | 30 % | 30 % | ISO 4589 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ROA; IEC 60093 |
| Dielectric Constant | 2.7 @Frequency 1.00e+6 Hz |
2.7 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 2.9 @Frequency 50.0 - 60.0 Hz |
2.9 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
| Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
| Dissipation Factor | 0.0065 @Frequency 1.00e+6 Hz |
0.0065 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 0.015 @Frequency 50.0 - 60.0 Hz |
0.015 @Frequency 50.0 - 60.0 Hz |
IEC 60250 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 75°C +/- 2°C | PASSES | IEC 60695-10-2 |