Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics SABIC STAMAX 20YM240 PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name SABIC STAMAX
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics SABIC STAMAX 20YM240 PP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SABIC® STAMAX 20YM240 is a 20% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 62455287.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Filler Content 20 %
20 %
glass; ISO 3451
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
50 mm/min, 1A; ISO 527
45.0 MPa

@Temperature 120 °C
6530 psi

@Temperature 248 °F
50 mm/min, 1A; ISO 527
60.0 MPa

@Temperature 80.0 °C
8700 psi

@Temperature 176 °F
50 mm/min, 1A; ISO 527
Elongation at Break 2.5 %
2.5 %
50 mm/min; ISO 527
Tensile Modulus 4.80 GPa
696 ksi
1 mm/min; ISO 527
2.80 GPa

@Temperature 120 °C
406 ksi

@Temperature 248 °F
1 mm/min; ISO 527
3.40 GPa

@Temperature 80.0 °C
493 ksi

@Temperature 176 °F
1 mm/min; ISO 527
Flexural Modulus 4.10 GPa
595 ksi
2 mm/min, 64mm span; ISO 178
2.85 GPa

@Temperature 80.0 °C
413 ksi

@Temperature 176 °F
2 mm/min, 64mm span; ISO 178
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
80*10*4mm, Cut; ISO 179/1eA
1.80 J/cm²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
80*10*4mm, Cut; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 156 °C
313 °F
80*10*4mm, Cut; ISO 75-1&2