SABIC Innovative Plastics Ultem HFATX200 PEI+PCE

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI) + PCE
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Ultem HFATX200 PEI+PCE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D 792
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.50 %
0.50 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.90 %

@Temperature 23.0 °C
0.90 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
on tensile bar; SABIC Method
0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 8.0 g/10 min

@Load 6.60 kg,
Temperature 295 °C
8.0 g/10 min

@Load 14.6 lb,
Temperature 563 °F
ASTM D 1238
40 g/10 min

@Load 5.00 kg,
Temperature 340 °C
40 g/10 min

@Load 11.0 lb,
Temperature 644 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
66 g/10 min

@Load 6.60 kg,
Temperature 337 °C
66 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.0 MPa
11900 psi
Type I, 5 mm/min; ASTM D 638
84.0 MPa
12200 psi
5 mm/min; ISO 527
Tensile Strength, Yield 92.0 MPa
13300 psi
Type I, 5 mm/min; ASTM D 638
95.0 MPa
13800 psi
5 mm/min; ISO 527
Elongation at Break 20 %
20 %
Type I, 5 mm/min; ASTM D 638
27 %
27 %
5 mm/min; ISO 527
Elongation at Yield 6.7 %
6.7 %
5 mm/min; ISO 527
7.0 %
7.0 %
Type I, 5 mm/min; ASTM D 638
Tensile Modulus 2.90 GPa
421 ksi
5 mm/min; ASTM D 638
3.08 GPa
447 ksi
1 mm/min; ISO 527
Flexural Yield Strength 138 MPa
20000 psi
2 mm/min; ISO 178
146 MPa
21200 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.95 GPa
428 ksi
2 mm/min; ISO 178
3.20 GPa
464 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 0.450 J/cm

@Temperature -30.0 °C
0.843 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
15.0 J/cm

@Thickness 3.20 mm
28.1 ft-lb/in

@Thickness 0.126 in
reverse notched; ASTM D 256
Izod Impact, Notched (ISO) 4.00 kJ/m²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 125 kJ/m²

@Temperature -30.0 °C
59.5 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
131 kJ/m²

@Temperature 23.0 °C
62.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 11.5 J/cm²

@Temperature -30.0 °C
54.7 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
18.0 J/cm²

@Temperature 23.0 °C
85.7 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Impact Test 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 53.0 µm/m-°C

@Temperature -40.0 - 150 °C
29.4 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
53.0 µm/m-°C

@Temperature 23.0 - 150 °C
29.4 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow 53.0 µm/m-°C

@Temperature -40.0 - 150 °C
29.4 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
53.0 µm/m-°C

@Temperature 23.0 - 150 °C
29.4 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 199 °C

@Thickness 3.20 mm
390 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
180 °C

@Thickness 3.20 mm
356 °F

@Thickness 0.126 in
unannealed; ASTM D 648
186 °C

@Thickness 6.40 mm
367 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Vicat Softening Point 192 °C
378 °F
Rate B/50; ISO 306
201 °C
394 °F
Rate B/120; ISO 306
201 °C
394 °F
Rate B/50; ASTM D 1525
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C Passes
IEC 60695-10-2