Teijin Panlite® K-1300Y Standard (mold release/ice color grade) Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Teijin
Trade Name Panlite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teijin Panlite® K-1300Y Standard (mold release/ice color grade) Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Extrusion molding, blow molding and thick-wall injection molding grade. It has a improved mold release property and is bluish-tinted to exhibit clear color.Applications:Extruded products such as sheets, films, pipes and profilesDirect-blow and injection-blow moldings such as bottles, tanks and containesrRotational forming products such as large-size tanks and large-size containers.Information provided by Teijin Chemicals Ltd.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption 0.20 %
0.20 %
in water, 23°C, 24h; ISO 62
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm

@Thickness 4.00 mm
0.0050 - 0.0070 in/in

@Thickness 0.157 in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 4.00 mm
0.0050 - 0.0070 in/in

@Thickness 0.157 in
Melt Flow 3.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
3.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
50mm/min; ISO 527
Elongation at Break >= 50 %
>= 50 %
50mm/min; ISO 527
Elongation at Yield 6.0 %
6.0 %
50mm/min; ISO 527
Tensile Modulus 2.35 GPa
341 ksi
1mm/min; ISO 527
Flexural Strength 90.0 MPa
13100 psi
2mm/min; ISO 178
Flexural Modulus 2.20 GPa
319 ksi
2mm/min; ISO 178
Charpy Impact Unnotched NB
NB
ISO 179
Charpy Impact, Notched 8.90 J/cm²
42.4 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
ISO 11359
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
ISO 75
Vicat Softening Point 151 °C
304 °F
50°C/hr, 50N; ISO 306
UL RTI, Electrical 125 °C

@Thickness 1.47 mm
257 °F

@Thickness 0.0579 in
UL 746B
UL RTI, Mechanical with Impact 115 °C

@Thickness 1.47 mm
239 °F

@Thickness 0.0579 in
UL 746B
UL RTI, Mechanical without Impact 125 °C

@Thickness 1.47 mm
257 °F

@Thickness 0.0579 in
UL 746B
Flammability, UL94 HB

@Thickness 0.380 mm
HB

@Thickness 0.0150 in
Optical Properties Metric English Comments
Refractive Index 1.585
1.585
ASTM D542
Transmission, Visible 88 %

@Thickness 3.00 mm
88 %

@Thickness 0.118 in
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Dielectric Constant 3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
IEC 60250
3.1

@Frequency 100 Hz
3.1

@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243
Dissipation Factor 0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
IEC 60250
0.0090

@Frequency 1e+6 Hz
0.0090

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 V
250 V
IEC 60112