| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
| Water Absorption | 1.4 % @Time 86400 sec |
1.4 % @Time 24.0 hour |
ISO 62 |
| Moisture Absorption at Equilibrium | 2.1 % | 2.1 % | 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
|
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 98 | 98 | ISO 2039 |
| Tensile Strength at Break | 47.0 MPa | 6820 psi | ISO 527-1/-2 |
| Elongation at Break | 4.8 % | 4.8 % | ISO 527-1/-2 |
| Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
| Flexural Strength | 60.0 MPa | 8700 psi | ISO 178 |
| Flexural Modulus | 2.20 GPa | 319 ksi | ISO 178 |
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179-1 |
| Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-2 |
| Flammability, UL94 | HB @Thickness 0.750 mm |