Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.15 - 1.61 g/cc | 0.0415 - 0.0582 lb/in³ | Average value: 1.42 g/cc Grade Count:27 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Density | 1.39 - 1.61 g/cc | 0.0502 - 0.0582 lb/in³ | Average value: 1.50 g/cc Grade Count:17 |
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an.. |
|||
Density | 1.58 - 1.61 g/cc | 0.0571 - 0.0582 lb/in³ | Average value: 1.60 g/cc Grade Count:5 |
Overview of materials for Polyamide-Imide, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.47 - 1.61 g/cc | 0.0531 - 0.0582 lb/in³ | Average value: 1.52 g/cc Grade Count:12 |
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and .. |
|||
Density | 1.11 - 1.61 g/cc | 0.0401 - 0.0582 lb/in³ | Average value: 1.39 g/cc Grade Count:37 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Density | 1.29 - 1.61 g/cc | 0.0466 - 0.0582 lb/in³ | Average value: 1.46 g/cc Grade Count:65 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Density | 1.57 - 1.61 g/cc | 0.0567 - 0.0582 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 88/3 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.28 - 1.61 g/cc | 0.0462 - 0.0582 lb/in³ | Average value: 1.43 g/cc Grade Count:102 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Density | 1.57 - 1.61 g/cc | 0.0567 - 0.0582 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 130 Rigid PVC, Extrusion Pipes and profiles |