Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chesterton ARC S2 Ceramic reinforced erosion resistant coating

Category Ceramic , Polymer , Thermoset , Epoxy
Manufacturer Chesterton
Trade Name ARC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton ARC S2 Ceramic reinforced erosion resistant coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. ARC S2 is formulated for the resurfacing of metal components subjected to extreme corrosive or severe fluid flow conditions. ARC S2 is a low viscosity composite that is designed to be spray applied but may also be applied by roller or brush. This product is formulated as a two coat system to provide extended wear life for plant equipment. Cured ARC S2 provides a high gloss ceramic surface with resistance to erosion-corrosion.Benefits:High gloss finish reduces drag, improves pump efficiency on worn componentsTough resin structure resists thermal-mechanical shockOutstanding adhesion insures reliable performance against under film corrosionLabor and downtime are reduced due to ease of application and rapid curingConvenient 2-1 volumetric mix ratio and verification of mix by color changePerforms well under fluctuating chemical environments. Suggested Uses:Fans & HousingsHeat ExchangersHoppersTank LiningsValve AssembliesWaterboxesCooling Water SystemsPump ComponentsScrubber SystemsPipeline CoatingsInformation provided by Chesterton
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Cured
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength at Break 46.2 MPa
6700 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 5.45 GPa
790 ksi
ASTM D790
Compressive Strength 64.8 MPa
9400 psi
ASTM D695
Adhesive Bond Strength >= 14.5 MPa
>= 2100 psi
Lap Shear; ASTM D4541
Taber Abrasion, mg/1000 Cycles 280

@Load 1.00 kg
280

@Load 2.20 lb
H-18, (loss); ASTM D4060
Abrasion 2.4
2.4
[%], Weight Loss, Jet Abrasion; Federal Test method Spec. 6193 Modified
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 52.0 °C
126 °F
Wet Service
80.0 °C
176 °F
Dry Service
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 32.0 °C
1.00 hour

@Temperature 89.6 °F
Tack Free
120 min

@Temperature 25.0 °C
2.00 hour

@Temperature 77.0 °F
Tack Free
180 min

@Temperature 16.0 °C
3.00 hour

@Temperature 60.8 °F
Tack Free
300 min

@Temperature 32.0 °C
5.00 hour

@Temperature 89.6 °F
Light Load
360 min

@Temperature 10.0 °C
6.00 hour

@Temperature 50.0 °F
Tack Free
600 min

@Temperature 25.0 °C
10.0 hour

@Temperature 77.0 °F
Light Load
600 min

@Temperature 32.0 °C
10.0 hour

@Temperature 89.6 °F
Overcoat End
840 min

@Temperature 32.0 °C
14.0 hour

@Temperature 89.6 °F
Full Load
1080 min

@Temperature 16.0 °C
18.0 hour

@Temperature 60.8 °F
Light Load
1200 min

@Temperature 25.0 °C
20.0 hour

@Temperature 77.0 °F
Overcoat End
1440 min

@Temperature 10.0 °C
24.0 hour

@Temperature 50.0 °F
Light Load
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Full Load
1440 min

@Temperature 32.0 °C
24.0 hour

@Temperature 89.6 °F
Full Chemical
1800 min

@Temperature 16.0 °C
30.0 hour

@Temperature 60.8 °F
Overcoat End
2400 min

@Temperature 10.0 °C
40.0 hour

@Temperature 50.0 °F
Overcoat End
2880 min

@Temperature 16.0 °C
48.0 hour

@Temperature 60.8 °F
Full Load
2880 min

@Temperature 25.0 °C
48.0 hour

@Temperature 77.0 °F
Full Chemical
3600 min

@Temperature 10.0 °C
60.0 hour

@Temperature 50.0 °F
Full Load
5760 min

@Temperature 16.0 °C
96.0 hour

@Temperature 60.8 °F
Full Chemical
7200 min

@Temperature 10.0 °C
120 hour

@Temperature 50.0 °F
Full Chemical
Descriptive Properties Value Comments
Color Gray
Green
Copyright © lookpolymers.com All Rights Reserved