Plastcom SLOVAMID 66 C 15 MI PA66, 15% mineral filling

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Mineral Filled, Impact Grade
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 66
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 66 C 15 MI PA66, 15% mineral filling.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Viscosity Measurement 1.34 - 1.37
1.34 - 1.37
Linear Mold Shrinkage 0.0134 cm/cm
0.0134 in/in
Linear Mold Shrinkage, Transverse 0.0137 cm/cm
0.0137 in/in
Melt Flow 3.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
3.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 52.0 MPa
7540 psi
Elongation at Break 5.0 %
5.0 %
Tensile Modulus 3.80 GPa
551 ksi
Flexural Strength 245 MPa
35500 psi
Flexural Modulus 3.65 GPa
529 ksi
Charpy Impact Unnotched 2.50 J/cm²

@Temperature -20.0 °C
11.9 ft-lb/in²

@Temperature -4.00 °F
7.50 J/cm²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.100 J/cm²

@Temperature -20.0 °C
0.476 ft-lb/in²

@Temperature -4.00 °F
0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Vicat Softening Point 260 °C
500 °F
B
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
Dielectric Strength 40.0 kV/mm
1020 kV/in
Comparative Tracking Index 500 V
500 V
Processing Properties Metric English Comments
Melt Temperature 280 - 310 °C
536 - 590 °F
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Drying Temperature 100 °C
212 °F
Dry Time 4 hour
4 hour
Moisture Content 0.20 %
0.20 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi