Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphthalate Carbonate
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam sterilizable.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption 0.16 %

@Time 86400 sec
0.16 %

@Time 24.0 hour
ASTM D570
Moisture Absorption 0.350 %
0.350 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.16 %
0.16 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0070 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 3.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
3.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 3.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
3.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
12 g/10 min

@Load 2.16 kg,
Temperature 330 °C
12 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength at Break 65.0 MPa
9430 psi
50 mm/min; ISO 527
71.0 MPa
10300 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa
9430 psi
Type I, 50 mm/min; ASTM D638
65.0 MPa
9430 psi
50 mm/min; ISO 527
Elongation at Break 7.0 %
7.0 %
50 mm/min; ISO 527
122 %
122 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
Type I, 50 mm/min; ASTM D638
7.0 %
7.0 %
50 mm/min; ISO 527
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D638
2.26 GPa
328 ksi
1 mm/min; ISO 527
Flexural Yield Strength 66.0 MPa
9570 psi
2 mm/min; ISO 178
95.0 MPa
13800 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.02 GPa
293 ksi
1.3 mm/min, 50 mm span; ASTM D790
2.12 GPa
307 ksi
2 mm/min; ISO 178
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
1.44 J/cm

@Temperature -30.0 °C
2.70 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 32.04 J/cm
60.02 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
11.0 kJ/m²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Tensile Impact Strength 577 kJ/m²
275 ft-lb/in²
Type S; ASTM D1822
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
73.0 J

@Temperature 23.0 °C
53.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
91.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
51.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Specific Heat Capacity 1.26 J/g-°C
0.301 BTU/lb-°F
ASTM C351
Thermal Conductivity 0.210 W/m-K
1.46 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
143 °C

@Thickness 3.20 mm
289 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 154 °C
309 °F
Rate B/50; ISO 306
155 °C
311 °F
Rate B/120; ISO 306
160 °C
320 °F
Rate B/50; ASTM D1525
UL RTI, Electrical 125 °C
257 °F
UL 746B
UL RTI, Mechanical with Impact 125 °C
257 °F
UL 746B
UL RTI, Mechanical without Impact 125 °C
257 °F
UL 746B
Optical Properties Metric English Comments
Refractive Index 1.60
1.60
ASTM D542
Haze 1.0 %

@Thickness 2.54 mm
1.0 %

@Thickness 0.100 in
ASTM D1003
Transmission, Visible 85 %
85 %
2.54 mm; ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity >= 2.60e+17 ohm-cm
>= 2.60e+17 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
ASTM D150
3.15

@Frequency 50.0 - 60.0 Hz
3.15

@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 20.3 kV/mm

@Thickness 3.20 mm
516 kV/in

@Thickness 0.126 in
in air; ASTM D149
Dissipation Factor 0.0012

@Frequency 50.0 - 60.0 Hz
0.0012

@Frequency 50.0 - 60.0 Hz
ASTM D150
0.024

@Frequency 100 Hz
0.024

@Frequency 100 Hz
ASTM D150
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
0.00 - 15 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
Descriptive Properties Value Comments
Specific Volume 0.83cm^3/g
ASTM D792
Users viewing this material also viewed the following: