| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Extruded |
| Manufacturer | Covestro |
| Trade Name | Makrolon® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Covestro Makrolon® 1804 Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| 1.02 g/cc @Temperature 300 °C |
0.0368 lb/in³ @Temperature 572 °F |
Melt | |
| Water Absorption | 0.30 % | 0.30 % | Similar to ISO 62 |
| Moisture Absorption at Equilibrium | 0.12 % | 0.12 % | Similar to ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
| Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | ISO 294-4,2577 |
| Melt Flow | 6.1 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.1 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 65.0 MPa | 9430 psi | ISO 527-1/-2 |
| Elongation at Break | >= 50 % | >= 50 % | Nominal; ISO 527-1/-2 |
| Elongation at Yield | 6.2 % | 6.2 % | ISO 527-1/-2 |
| Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | NB | NB | ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179/1eU | |
| Impact | 5600 | 5600 | Puncture - maximum force (N); ISO 6603-2 |
| 6500 @Temperature -30.0 °C |
6500 @Temperature -22.0 °F |
Puncture - maximum force (N); ISO 6603-2 | |
| Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
| 70.0 J @Temperature -30.0 °C |
51.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 | |
| Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
| Tensile Creep Modulus, 1000 hours | 1900 MPa | 276000 psi | ISO 899-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
| Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
| Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
| Deflection Temperature at 0.46 MPa (66 psi) | 140 °C | 284 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 128 °C | 262 °F | ISO 75-1/-2 |
| Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
| Glass Transition Temp, Tg | 148 °C | 298 °F | ISO 11357-1/-2 |
| Flammability, UL94 | V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
IEC 60695-11-10 |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
IEC 60695-11-10 | |
| Oxygen Index | 30 % | 30 % | ISO 4589-1/-2 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 89 % | 89 % | ISO 13468-1, -2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
| Dielectric Constant | 3.0 @Frequency 1.00e+6 Hz |
3.0 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.1 @Frequency 100 Hz |
3.1 @Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.00050 @Frequency 100 Hz |
0.00050 @Frequency 100 Hz |
IEC 60250 |
| 0.0095 @Frequency 1.00e+6 Hz |
0.0095 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
| 300 °C | 572 °F | Injection Molding; ISO 294 | |
| Mold Temperature | 80.0 °C | 176 °F | Injection Molding; ISO 10724 |
| 80.0 - 120 °C | 176 - 248 °F | ||
| Ejection Temperature | 130 °C | 266 °F | |
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Availability | North America | |
| Eff. thermal diffusivity (m²/s) | 1E-07 | |
| Feature | Light stabilised or stable to light | |
| U.V. stabilised or stable to weather | ||
| Form | Pellets | |
| Process | Other Extrusion | |
| Profile Extrusion | ||
| Sheet Extrusion |