| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
| 1.02 g/cc @Temperature 290 °C |
0.0368 lb/in³ @Temperature 554 °F |
Melt | |
| Water Absorption | 0.40 % | 0.40 % | Similar to ISO 62 |
| Moisture Absorption at Equilibrium | 0.12 % | 0.12 % | Similar to ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
| Melt Flow | 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
11 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 58.0 MPa | 8410 psi | ISO 527-1/-2 |
| Elongation at Break | >= 50 % | >= 50 % | Nominal; ISO 527-1/-2 |
| Elongation at Yield | 5.7 % | 5.7 % | ISO 527-1/-2 |
| Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | NB | NB | ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179/1eU | |
| Impact | 4900 | 4900 | Puncture - maximum force (N); ISO 6603-2 |
| 5800 @Temperature -30.0 °C |
5800 @Temperature -22.0 °F |
Puncture - maximum force (N); ISO 6603-2 | |
| Puncture Energy | 50.0 J | 36.9 ft-lb | ISO 6603-2 |
| 55.0 J @Temperature -30.0 °C |
40.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
| Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
| Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
| Deflection Temperature at 0.46 MPa (66 psi) | 134 °C | 273 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 122 °C | 252 °F | ISO 75-1/-2 |
| Vicat Softening Point | 142 °C | 288 °F | 50°C/h 50N; ISO 306 |
| Flammability, UL94 | HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
IEC 60695-11-10 |
| Oxygen Index | 30 % | 30 % | ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
| Dielectric Constant | 3.1 @Frequency 1.00e+6 Hz |
3.1 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.2 @Frequency 100 Hz |
3.2 @Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.0012 @Frequency 100 Hz |
0.0012 @Frequency 100 Hz |
IEC 60250 |
| 0.012 @Frequency 1.00e+6 Hz |
0.012 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 290 °C | 554 °F | Injection Molding; ISO 294 |
| 280 - 320 °C | 536 - 608 °F | ||
| Mold Temperature | 80.0 °C | 176 °F | Injection Molding; ISO 10724 |
| 80.0 - 120 °C | 176 - 248 °F | ||
| Ejection Temperature | 130 °C | 266 °F | |
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Availability | Asia Pacific | |
| Europe | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Eff. thermal diffusivity (m²/s) | 1E-07 | |
| Feature | Release agent | |
| Form | Pellets | |
| Process | Injection Molding |