| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Crastin® SK601 BK851 PBT
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
| Filler Content | 10 % | 10 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 87.0 MPa @Temperature 23.0 °C |
12600 psi @Temperature 73.4 °F |
ISO 527 |
| Elongation at Break | 4.0 % @Temperature 23.0 °C |
4.0 % @Temperature 73.4 °F |
ISO 527 |
| Tensile Modulus | 4.50 GPa @Temperature 23.0 °C |
653 ksi @Temperature 73.4 °F |
ISO 527 |
| Flexural Strength | 140 MPa @Temperature 23.0 °C |
20300 psi @Temperature 73.4 °F |
ISO 178 |
| Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
| Charpy Impact Unnotched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 225 °C | 437 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 180 °C | 356 °F | ISO 75-1/-2 |
| UL RTI, Electrical | 130 °C @Thickness 6.00 mm |
266 °F @Thickness 0.236 in |
UL 746B |
| 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
UL 746B | |
| 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B | |
| 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
UL 746B | |
| UL RTI, Mechanical with Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746B |
| 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746B | |
| 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
UL 746B | |
| 115 °C @Thickness 6.00 mm |
239 °F @Thickness 0.236 in |
UL 746B | |
| UL RTI, Mechanical without Impact | 120 °C @Thickness 6.00 mm |
248 °F @Thickness 0.236 in |
UL 746B |
| 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
UL 746B | |
| 120 °C @Thickness 0.750 mm |
248 °F @Thickness 0.0295 in |
UL 746B | |
| 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746B | |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
IEC 60695-11-10 |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
IEC 60695-11-10 | |
| HB @Thickness 6.00 mm |
HB @Thickness 0.236 in |
IEC 60695-11-10 | |
| HB @Thickness 6.00 mm |
HB @Thickness 0.236 in |
UL94 | |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
UL94 | |
| HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
UL94 | |
| Oxygen Index | 20 % | 20 % | ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 250 V @Temperature 23.0 °C |
250 V @Temperature 73.4 °F |
UL 746A |
| 300 V @Temperature 23.0 °C |
300 V @Temperature 73.4 °F |
IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 250 °C | 482 °F | Optimum |
| 240 - 260 °C | 464 - 500 °F | ||
| Mold Temperature | 80.0 °C | 176 °F | optimum |
| 30.0 - 130 °C | 86.0 - 266 °F | ||
| Drying Temperature | 110 - 130 °C | 230 - 266 °F | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
| Moisture Content | <= 0.040 % | <= 0.040 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Lubricant | |
| Appearance | Black Color | |
| Drying Recommended | Yes | |
| Features | Chemical Resistance, Good | |
| Dimensional Stability, Good | ||
| Lubricated | ||
| Moisture Absorption, Low | ||
| Processability, Good | ||
| Stiffness, Good | ||
| Strength, Good | ||
| Filler | Glass fiber reinforcement | |
| Forms | Pellets | |
| Generic | PBT | |
| Material Status | Current | |
| Part Marking Code | >PBT-GF10< | ISO 11469 |
| Polymer Family | Polyester | |
| Polymer Type | PBT | |
| Processing Method | Injection Molding | |
| Product Category | Glass Reinforced Resins | |
| Region Available - Global | Yes | |
| Resin Identification | PBT-GF10 | ISO 1043 |
| RoHS Compliance | Contact Manufacturer | |
| Uses | Automotive Applications | |
| General Purpose | ||
| Industrial Applications | ||
| Parts, Engineering | ||
| Parts, Machine/Mechanical | ||
| Structural Parts |