| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.39 g/cc | 0.0502 lb/in³ | DAM; ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 140 MPa | 20300 psi | 50%RH; ISO 527-1/-2 |
| 200 MPa | 29000 psi | DAM; ISO 527-1/-2 | |
| Elongation at Break | 3.0 % | 3.0 % | DAM; ISO 527-1/-2 |
| 4.0 % | 4.0 % | 50%RH; ISO 527-1/-2 | |
| Tensile Modulus | 8.00 GPa | 1160 ksi | 50%RH; ISO 527-1/-2 |
| 10.5 GPa | 1520 ksi | DAM; ISO 527-1/-2 | |
| Flexural Strength | 195 MPa | 28300 psi | 50%RH; ISO 178 |
| 280 MPa | 40600 psi | DAM; ISO 178 | |
| Flexural Modulus | 9.30 GPa | 1350 ksi | DAM; ISO 178 |
| Izod Impact, Notched (ISO) | 12.0 kJ/m² | 5.71 ft-lb/in² | DAM; ISO 180/1A |
| 10.0 kJ/m² @Temperature -40.0 °C |
4.76 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A | |
| Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | DAM; ISO 179/1eU |
| 8.00 J/cm² | 38.1 ft-lb/in² | 50%RH; ISO 179/1eU | |
| Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | DAM; ISO 179/1eA |
| 1.30 J/cm² | 6.19 ft-lb/in² | 50%RH; ISO 179/1eA | |
| 1.00 J/cm² @Temperature -40.0 °C |
4.76 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 18.0 µm/m-°C | 10.0 µin/in-°F | DAM; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 83.0 µm/m-°C | 46.1 µin/in-°F | DAM; ISO 11359-1/-2 |
| Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 252 °C | 486 °F | DAM; ISO 75-1/-2 |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; IEC 60695-11-10 |
| HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
DAM; IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 400 V | 400 V | DAM; IEC 60112 |
| 400 - 600 V | 400 - 600 V | DAM; UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Part Marking Code | >PA66-GF33< | ISO 11469 |
| Processing | Injection Moulding | |
| Regional Availability | Asia Pacific | |
| Europe | ||
| Global | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Resin Identification | PA66-GF33 | |
| Special Characteristics | Heat stabilised or stable to heat | |
| UL recognition | UL | DAM |