| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | DAM; ISO 1183 |
| Water Absorption | 2.6 % @Temperature 23.0 °C |
2.6 % @Temperature 73.4 °F |
Equilibrium 50%RH; DAM; ISO 62, Similar to |
| 8.5 % @Temperature 23.0 °C |
8.5 % @Temperature 73.4 °F |
Saturation, immersed; DAM; ISO 62, Similar to | |
| Linear Mold Shrinkage | 0.015 cm/cm @Thickness 3.20 mm |
0.015 in/in @Thickness 0.126 in |
Flow; DAM |
| Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 55.0 MPa @Temperature 23.0 °C |
7980 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 83.0 MPa @Temperature 23.0 °C |
12000 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Elongation at Break | >= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
DAM; nominal; ISO 527 |
| >= 100 % @Temperature 23.0 °C |
>= 100 % @Temperature 73.4 °F |
50%RH; nominal; ISO 527 | |
| Elongation at Yield | 4.4 % @Temperature 23.0 °C |
4.4 % @Temperature 73.4 °F |
DAM; ISO 527 |
| 27 % @Temperature 23.0 °C |
27 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| Tensile Modulus | 1.30 GPa @Temperature 23.0 °C |
189 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 3.10 GPa @Temperature 23.0 °C |
450 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Flexural Modulus | 1.07 GPa @Temperature 23.0 °C |
155 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
| 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
DAM; ISO 178 | |
| Izod Impact, Notched (ISO) | 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A |
| 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A | |
| 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A | |
| 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
50%RH; ISO 180/1U |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
DAM; ISO 180/1U | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
DAM; ISO 180/1U | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
50%RH; ISO 180/1U | |
| Charpy Impact Unnotched | NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
DAM; ISO 179/1eU | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
50%RH; ISO 179/1eU | |
| Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
| 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
| 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA | |
| 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 23.0 - 55.0 °C |
278 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
| Melting Point | 262 °C | 504 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | DAM; ISO 75-1/-2 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 285 °C | 545 °F | DAM; Optimum; Extrusion |
| 280 - 290 °C | 536 - 554 °F | DAM; Extrusion | |
| 280 - 300 °C | 536 - 572 °F | DAM; Injection Molding | |
| 290 °C | 554 °F | DAM; Optimum; Injection Molding | |
| Mold Temperature | 70.0 °C | 158 °F | DAM; optimum; Injection Molding |
| 50.0 - 90.0 °C | 122 - 194 °F | DAM; Injection Molding | |
| Drying Temperature | 80.0 °C | 176 °F | DAM; Extrusion |
| 80.0 °C | 176 °F | DAM; Injection Molding | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM; Injection Molding |
| 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Extrusion | |
| Moisture Content | <= 0.050 % | <= 0.050 % | DAM; Extrusion |
| <= 0.050 % | <= 0.050 % | DAM; Injection Molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | DAM |
| Features | Food Contact Acceptable | DAM |
| Viscosity, High | DAM | |
| Forms | Pellets | DAM |
| Generic | Nylon 66 | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA66< | ISO 11469; DAM |
| Processing Method | Extrusion | DAM |
| Product Category | Extrusion Resins | DAM |
| Food Contact Resins | DAM | |
| Unreinforced Resins | DAM | |
| Resin Identification | PA66 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |
| Uses | Food Applications, Non-specific | DAM |