| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Impact Modified , Polycarbonate, Unreinforced, Flame Retardant |
| Manufacturer | Eurotec |
| Trade Name | Tecotek® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.200 % @Temperature 23.0 °C |
0.200 % @Temperature 73.4 °F |
50% RH; ISO 960 |
| Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | Eurotec |
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | Eurotec |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 60.0 MPa | 8700 psi | ISO 527 |
| Elongation at Break | >= 20 % | >= 20 % | ISO 527 |
| Tensile Modulus | 0.225 GPa | 32.6 ksi | ISO 527 |
| Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
| 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 180/1U |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 180/1U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | ISO 75 |
| Vicat Softening Point | 130 °C @Load 5.10 kg |
266 °F @Load 11.2 lb |
ISO 306 |
| Flammability, UL94 | V-0 @Thickness 0.750 mm |
V-0 @Thickness 0.0295 in |
|
| V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
||
| Glow Wire Test | 875 °C @Thickness 2.00 mm |
1610 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
| 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI; IEC 60695 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
| Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
| Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
| Drying Temperature | 120 °C | 248 °F | |
| Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
| Moisture Content | <= 0.10 % | <= 0.10 % | ISO 960 |
| Hold Pressure | 60.0 - 120 MPa | 8700 - 17400 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Injection Speed | Medium - Fast |