NextGen Adhesives G907-27 Structural Adhesive

Category Polymer , Adhesive
Manufacturer NextGen Adhesives
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF NextGen Adhesives G907-27 Structural Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: NGAC G907-27 is a medium viscosity polyamide adhesive system utilized extensively in industrial and structural applications.Advantages and Applications: The NGAC G907-27 provides excellent chemical, mechanical resistance, as well as, overall toughness. The NGAC G907-27 is easily mixed and cured at room temperature and provides excellent adhesion to glass, ceramic, metal and plastic.Information Provided by Nextgen Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Viscosity 37000 cP
37000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Shear Strength 13.8 MPa
2000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 - 4320 min

@Temperature 25.0 °C
24.0 - 72.0 hour

@Temperature 77.0 °F
Pot Life 60 min
60 min
Descriptive Properties Value Comments
Color Amber
Mix Ratio by Weight (R/H) 1