| Category | Polymer , Thermoplastic , Polyurethane, TP |
| Manufacturer | Plastcom spol. s r.o. |
| Trade Name | PLASTALEN® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Plastcom PLASTALEN® TPU N 85 LTS TPU.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | STN EN ISO 1183-1 |
| Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 200 °C |
10 g/10 min @Load 4.76 lb, Temperature 392 °F |
STN EN ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 45.0 MPa | 6530 psi | STN EN ISO 527-2 |
| Elongation at Break | 750 % | 750 % | STN EN ISO 527-2 |
| Tensile Modulus | 0.350 GPa | 50.8 ksi | STN EN ISO 527-2 |
| Flexural Strength | 14.0 MPa | 2030 psi | STN EN ISO 178 |
| Flexural Modulus | 0.160 GPa | 23.2 ksi | STN EN ISO 178 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
STN EN ISO 179 |
| NB @Temperature -20.0 °C |
NB @Temperature -4.00 °F |
STN EN ISO 179 | |
| Charpy Impact, Notched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
STN EN ISO 179 |
| NB @Temperature -20.0 °C |
NB @Temperature -4.00 °F |
STN EN ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 140 °C | 284 °F | STN EN 11357-1 |
| Vicat Softening Point | 130 °C | 266 °F | STN EN ISO 306 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 180 - 230 °C | 356 - 446 °F | |
| Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | |
| Drying Temperature | 80.0 °C @Time 21600 sec |
176 °F @Time 6.00 hour |
|
| Moisture Content | <= 0.20 % | <= 0.20 % | STN EN ISO 3344 |
| Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Black |