Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
(Dry)
Water Absorption 5.5 %
5.5 %
initially dry
Moisture Absorption at Equilibrium 1.3 %
1.3 %
initially dry
Viscosity Measurement 140
140
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
Elongation at Break 3.2 %
3.2 %
Tensile Modulus 10.5 GPa
1520 ksi
Charpy Impact Unnotched 6.20 J/cm²

@Temperature -30.0 °C
29.5 ft-lb/in²

@Temperature -22.0 °F
9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V