| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.19 g/cc | 1.19 g/cc | ASTM D792 |
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.100 % | 0.100 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.13 % | 0.13 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 53.0 MPa | 7690 psi | 50 mm/min; ISO 527 |
| 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 66.0 MPa | 9570 psi | 50 mm/min; ISO 527 |
| 67.0 MPa | 9720 psi | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Break | 55 % | 55 % | Type I, 50 mm/min; ASTM D638 |
| 56 % | 56 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 6.0 % | 6.0 % | Type I, 50 mm/min; ASTM D638 |
| 6.0 % | 6.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
| 2.52 GPa | 365 ksi | 50 mm/min; ASTM D638 | |
| Flexural Yield Strength | 101 MPa | 14600 psi | 2 mm/min; ISO 178 |
| 107 MPa | 15500 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
| 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Unnotched | NB | NB | ASTM D4812 |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ASTM D4812 | |
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*3; ISO 180/1A |
| 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB | NB | 80*10*3; ISO 180/1U |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
80*10*3; ISO 180/1U | |
| Charpy Impact Unnotched | NB | NB | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
| Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 64.0 J @Temperature 23.0 °C |
47.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 77.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
42.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 79.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 131 °C | 268 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| 131 °C @Thickness 3.20 mm |
268 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 120 °C | 248 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 120 °C @Thickness 3.20 mm |
248 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 136 °C | 277 °F | Rate B/50; ASTM D1525 |
| 137 °C | 279 °F | Rate B/50; ISO 306 | |
| 139 °C | 282 °F | Rate B/120; ISO 306 | |
| UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
| UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
| UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
| Flammability, UL94 | V-2 @Thickness 0.400 mm |
V-2 @Thickness 0.0157 in |
UL 94 |
| V-1 @Thickness 1.00 mm |
V-1 @Thickness 0.0394 in |
UL 94 | |
| V-0 @Thickness 1.20 mm |
V-0 @Thickness 0.0472 in |
UL 94 | |
| 5VA @Thickness 3.00 mm |
5VA @Thickness 0.118 in |
UL 94 | |
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
| 960 °C @Thickness 1.20 mm |
1760 °F @Thickness 0.0472 in |
IEC 60695-2-12 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | >= 91 % | >= 91 % | 2.54 mm; ASTM D1003 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 2.79 @Frequency 1.00e+9 Hz |
2.79 @Frequency 1.00e+9 Hz |
ASTM ES 7-83 |
| Dissipation Factor | 0.0057 @Frequency 1.10e+9 Hz |
0.0057 @Frequency 1.10e+9 Hz |
ASTM ES 7-83 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | Pass | IEC 60695-10-2 |
| UV-light, water exposure/immersion | F1 | UL 746C |