| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics NORYL NH5120C PPE+PS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
| Density | 1.08 g/cc | 0.0390 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.0500 % | 0.0500 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.25 % | 0.25 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 20.6 g/10 min @Load 5.00 kg, Temperature 300 °C |
20.6 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
| Melt Index of Compound | 21 g/10 min @Load 5.00 kg, Temperature 300 °C |
21 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 54.0 MPa | 7830 psi | Type I, 50 mm/min; ASTM D638 |
| 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 64.0 MPa | 9280 psi | 50 mm/min; ISO 527 |
| 68.0 MPa | 9860 psi | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Break | 12.5 % | 12.5 % | 50 mm/min; ISO 527 |
| 13 % | 13 % | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Yield | 4.3 % | 4.3 % | 50 mm/min; ISO 527 |
| 4.5 % | 4.5 % | Type I, 50 mm/min; ASTM D638 | |
| Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
| 2.70 GPa | 392 ksi | 5 mm/min; ASTM D638 | |
| Flexural Yield Strength | 101 MPa | 14600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 103 MPa | 14900 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 2.58 GPa | 374 ksi | 2 mm/min; ISO 178 |
| 2.65 GPa | 384 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 2.28 J/cm | 4.27 ft-lb/in | ASTM D256 |
| 1.45 J/cm @Temperature -30.0 °C |
2.72 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
| 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 50.0 J @Temperature 23.0 °C |
36.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 76.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 76.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 7.50 µm/m-°C @Temperature -40.0 - 40.0 °C |
4.17 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 75.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 118 °C @Thickness 3.20 mm |
244 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 137 °C | 279 °F | Rate B/50; ASTM D1525 |
| 137 °C | 279 °F | Rate B/50; ISO 306 | |
| 139 °C | 282 °F | Rate B/120; ISO 306 | |
| UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
| UL RTI, Mechanical without Impact | 65.0 °C | 149 °F | UL 746B |
| Flammability, UL94 | V-1 @Thickness 1.50 mm |
V-1 @Thickness 0.0591 in |
UL 94 by SABIC-IP |