| Category | Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled |
| Manufacturer | Solvay Specialty Polymers |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Solvay Specialty Polymers Ryton® XE4050BL Polyphenylene Sulfide Alloy (PPS Alloy), GlassMineral Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D792 |
| Water Absorption | 0.050 % @Time 86400 sec |
0.050 % @Time 24.0 hour |
ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0020 cm/cm @Thickness 3.18 mm |
0.0020 in/in @Thickness 0.125 in |
|
| Linear Mold Shrinkage, Transverse | 0.0040 cm/cm @Thickness 3.20 mm |
0.0040 in/in @Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 74 | 74 | ASTM D785 |
| Hardness, Rockwell R | 110 | 110 | ASTM D785 |
| Tensile Strength | 124 MPa | 18000 psi | ASTM D638 |
| Tensile Stress | 135 MPa | 19600 psi | ISO 527-2 |
| Elongation at Break | 1.9 % | 1.9 % | ISO 527-2 |
| 1.9 % | 1.9 % | ASTM D638 | |
| Flexural Strength | 186 MPa | 27000 psi | ASTM D790 |
| 195 MPa | 28300 psi | ISO 178 | |
| Flexural Modulus | 10.0 GPa | 1450 ksi | ISO 178 |
| 10.3 GPa | 1490 ksi | ASTM D790 | |
| Compressive Strength | 200 MPa | 29000 psi | ASTM D695 |
| Poissons Ratio | 0.37 | 0.37 | ASTM E132 |
| Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Izod Impact, Unnotched | 6.40 J/cm @Thickness 3.18 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | Notch A; ISO 180 |
| Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | ISO 180 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 10.0 µm/m-°C @Temperature 100 - 200 °C |
5.56 µin/in-°F @Temperature 212 - 392 °F |
2 |
| 20.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
11.1 µin/in-°F @Temperature -58.0 - 122 °F |
2 | |
| CTE, linear, Transverse to Flow | 50.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
27.8 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
| 85.0 µm/m-°C @Temperature 100 - 200 °C |
47.2 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 | |
| Thermal Conductivity | 0.370 W/m-K | 2.57 BTU-in/hr-ft²-°F | ASTM C177 |
| Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | Unannealed; ASTM D648 |
| Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
|
| Oxygen Index | 25 % | 25 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Insulation Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
IEC 60167 |
| Dielectric Constant | 4.2 @Frequency 1.00e+6 Hz |
4.2 @Frequency 1.00e+6 Hz |
ASTM D150 |
| 4.3 @Frequency 1000 Hz |
4.3 @Frequency 1000 Hz |
ASTM D150 | |
| Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D149 |
| Dissipation Factor | 0.0030 @Frequency 1000 Hz |
0.0030 @Frequency 1000 Hz |
ASTM D150 |
| 0.0080 @Frequency 1.00e+6 Hz |
0.0080 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| Arc Resistance | 130 sec | 130 sec | ASTM D495 |
| Comparative Tracking Index | 150 V | 150 V | UL 746 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Availability | Asia Pacific | |
| Europe | ||
| Latin America | ||
| North America | ||
| Color | Black | |
| Form | Pellets | |
| RoHS Compliance | RoHS Compliant |