Material Notes:
Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron and steel gas mains. The excellent performance, especially creep and chemical resistance UBESTA supports industry as one of the most reliable materials.Comments: heat resistance, black colorInformation provided by UBE.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 235 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ASTM D1238R
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength at Break >= 56.0 MPa
>= 8120 psi
ASTM D638
Tensile Strength, Yield 46.0 MPa
6670 psi
ASTM D638
Elongation at Break >= 250 %
>= 250 %
ASTM D638
Flexural Strength 61.0 MPa
8850 psi
ASTM D790
Flexural Modulus 1.59 GPa
231 ksi
ASTM D790
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 230 °C
446 °F
Flange Temperature for T-Die Cast Film Extrusion
Feed Temperature 40.0 °C
104 °F
Injection Molding
Zone 1 190 °C
374 °F
For T-Die Cast Film Extrusion
230 °C
446 °F
For 8x1 mm Tube Extrusion
Zone 2 210 °C
410 °F
For T-Die Cast Film Extrusion
225 °C
437 °F
For 8x1 mm Tube Extrusion
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
230 °C
446 °F
For T-Die Cast Film Extrusion
Zone 4 215 °C
419 °F
For 8x1 mm Tube Extrusion
Die Temperature 230 °C
446 °F
For T-Die Cast Film Extrusion
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Molding
Injection Velocity 100 mm/sec
3.94 in/sec
Injection Molding
Die Opening 0.0400 cm
0.0157 in
For T-Die Cast Film Extrusion
Roll Temperature 50.0 °C
122 °F
Chill Roll Temperature for T-Die Cast Film Extrusion
Drying Temperature 80.0 °C
176 °F
Option 1
100 °C
212 °F
Option 2
110 °C
230 °F
Option 3
Dry Time 2 - 4 hour
2 - 4 hour
Option 3
4 - 6 hour
4 - 6 hour
Option 2
6 - 8 hour
6 - 8 hour
Option 1
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
Hold Pressure 25.0 - 50.0 MPa
3630 - 7250 psi
Injection Molding
Back Pressure 5.00 MPa
725 psi
Injection Molding
Screw Speed 15 - 76 rpm
15 - 76 rpm
For 8x1 mm Tube Extrusion
Descriptive Properties Value Comments
C/R 3-3.5:1
For 8x1 mm Tube Extrusion
Calibrating Vacuum 100 mbar
For 8x1 mm Tube Extrusion
Calibration 9.95 mm
For 8x1 mm Tube Extrusion
Compression Ratio 2.5-3.5:1
Injection Molding
min 3:1
For 8x1 mm Tube Extrusion
Die Diameter 16 mm
For 8x1 mm Tube Extrusion
Die Width 300 mm
For T-Die Cast Film Extrusion
Extruder Barmag, Screw Diameter = 30 mm
For T-Die Cast Film Extrusion
Extruder Characteristics 65 mm screw diameter
For 8x1 mm Tube Extrusion
Film Thickness 60 microns
For T-Die Cast Film Extrusion
Flight Depth in the Feeding Zone 10-15% of Screw Diameter
Injection Molding
Flight Depth in the Metering Zone 5-7% of Screw Diameter
Injection Molding
Haul Off Speed 5 m/min
For T-Die Cast Film Extrusion
Haul Speed 10-55 m/min
For 8x1 mm Tube Extrusion
L/D Ratio 25:1
For 8x1 mm Tube Extrusion
min 20:1
Injection Molding
Length of Compression Zone 25-45% of total screw length
Injection Molding
30% of screw length
For 8x1 mm Tube Extrusion
Length of Feeding Zone 20-40% of total screw length
Injection Molding
30-40% of screw length
For 8x1 mm Tube Extrusion
Length of Metering Zone 30-45% of screw length
For 8x1 mm Tube Extrusion
35-45% of total screw length
Injection Molding
Mandrel Diameter 12 mm
For 8x1 mm Tube Extrusion
Peripheral screw speed 10 m/min
Injection Molding
Water Temperature 10-18°C
For 8x1 mm Tube Extrusion