Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 4.76 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
0.952 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.50 kJ/m² Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Izod Impact, Notched (ISO) 4.00 - 10.0 kJ/m²
1.90 - 4.76 ft-lb/in²
Average value: 8.01 kJ/m² Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Izod Impact, Notched (ISO) 5.00 - 10.0 kJ/m²

@Temperature -40.0 - 30.0 °C
2.38 - 4.76 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 6.99 kJ/m² Grade Count:21
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Izod Impact, Notched (ISO) 9.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
4.28 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.67 kJ/m² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Izod Impact, Notched (ISO) 6.00 - 10.0 kJ/m²
2.86 - 4.76 ft-lb/in²
Average value: 7.91 kJ/m² Grade Count:11
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Izod Impact, Notched (ISO) 1.70 - 10.0 kJ/m²
0.809 - 4.76 ft-lb/in²
Average value: 3.22 kJ/m² Grade Count:13
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Izod Impact, Notched (ISO) 1.50 - 10.0 kJ/m²
0.714 - 4.76 ft-lb/in²
Average value: 6.68 kJ/m² Grade Count:11
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched (ISO) 3.00 - 10.0 kJ/m²
1.43 - 4.76 ft-lb/in²
Average value: 6.86 kJ/m² Grade Count:14
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Izod Impact, Notched (ISO) 4.00 - 10.0 kJ/m²
1.90 - 4.76 ft-lb/in²
Average value: 6.84 kJ/m² Grade Count:36
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Izod Impact, Notched (ISO) 4.00 - 10.0 kJ/m²

@Temperature -30.0 - 0.000 °C
1.90 - 4.76 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 6.80 kJ/m² Grade Count:9
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Izod Impact, Notched (ISO) 3.00 - 10.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 4.76 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 6.70 kJ/m² Grade Count:14
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Notched (ISO) 3.90 - 10.0 kJ/m²
1.86 - 4.76 ft-lb/in²
Average value: 7.17 kJ/m² Grade Count:8
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched (ISO) 4.00 - 10.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.90 - 4.76 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 7.31 kJ/m² Grade Count:4
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched (ISO) 3.00 - 10.0 kJ/m²

@Temperature -40.0 - -30.0 °C
1.43 - 4.76 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 5.65 kJ/m² Grade Count:15
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched (ISO) 6.50 - 10.0 kJ/m²
3.09 - 4.76 ft-lb/in²
Average value: 8.09 kJ/m² Grade Count:4
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Izod Impact, Notched (ISO) 3.00 - 10.0 kJ/m²
1.43 - 4.76 ft-lb/in²
Average value: 5.65 kJ/m² Grade Count:21
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Izod Impact, Notched (ISO) 3.00 - 10.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 4.76 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 5.09 kJ/m² Grade Count:9
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Izod Impact, Notched (ISO) 2.00 - 10.0 kJ/m²

@Temperature -30.0 - -20.0 °C
0.952 - 4.76 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 4.11 kJ/m² Grade Count:9
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched (ISO) 5.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
2.38 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.50 kJ/m² Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Izod Impact, Notched (ISO) 4.00 - 10.0 kJ/m²

@Temperature -40.0 - 0.000 °C
1.90 - 4.76 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 7.70 kJ/m² Grade Count:29
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched (ISO) 7.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.07 kJ/m² Grade Count:7
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Izod Impact, Notched (ISO) 7.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:3
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
Izod Impact, Notched (ISO) 8.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.33 kJ/m² Grade Count:2
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Izod Impact, Notched (ISO) 10.0 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
4.76 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 10.0 kJ/m² Grade Count:1
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
Izod Impact, Notched (ISO) 2.00 - 10.0 kJ/m²

@Temperature -30.0 - -20.0 °C
0.952 - 4.76 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 7.11 kJ/m² Grade Count:9
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Izod Impact, Notched (ISO) 2.00 - 10.0 kJ/m²
0.952 - 4.76 ft-lb/in²
Average value: 4.33 kJ/m² Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Izod Impact, Notched (ISO) 3.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
1.43 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.00 kJ/m² Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved