| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 79 | 79 | Conditioned; ISO 868 |
| 85 | 85 | ISO 868 | |
| Tensile Strength at Break | 65.0 MPa | 9430 psi | Conditioned; ISO R 527 |
| 70.0 MPa | 10200 psi | ISO R 527 | |
| Tensile Strength, Yield | 55.0 MPa | 7980 psi | Conditioned; ISO R 527 |
| 85.0 MPa | 12300 psi | ISO R 527 | |
| Elongation at Yield | 30 % | 30 % | ISO R 527 |
| >= 50 % | >= 50 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 1.30 GPa | 189 ksi | Conditioned; ISO 178 |
| 2.90 GPa | 421 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 4.50 kJ/m² | 2.14 ft-lb/in² | ISO 180/1A |
| 14.0 kJ/m² | 6.66 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | NB | NB | ISO 179/IeU |
| NB | NB | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/IeA |
| 1.30 J/cm² | 6.19 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | ASTM E831 |
| Melting Point | 260 °C | 500 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C | 194 °F | ISO 75-2/AF |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | Conditioned; CEI 60093 |
| 1.00e+15 ohm | 1.00e+15 ohm | CEI 60093 | |
| Comparative Tracking Index | 600 V | 600 V | CEI 60112/Solution A |