| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Crastin® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.17 g/cc | 0.0423 lb/in³ | |
| 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 | |
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Stress | 5.62 MPa @Strain 1.20 %, Temperature 90.0 °C |
815 psi @Strain 1.20 %, Temperature 194 °F |
ISO 11403-1 -2 |
| 12.17 MPa @Strain 3.20 %, Temperature 90.0 °C |
1765 psi @Strain 3.20 %, Temperature 194 °F |
ISO 11403-1 -2 | |
| 14.48 MPa @Strain 1.00 %, Temperature 40.0 °C |
2100 psi @Strain 1.00 %, Temperature 104 °F |
ISO 11403-1 -2 | |
| 16.27 MPa @Strain 0.800 %, Temperature 23.0 °C |
2360 psi @Strain 0.800 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
| 16.69 MPa @Strain 8.00 %, Temperature 90.0 °C |
2421 psi @Strain 8.00 %, Temperature 194 °F |
ISO 11403-1 -2 | |
| 18.44 MPa @Strain 0.800 %, Temperature 0.000 °C |
2675 psi @Strain 0.800 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
| 19.45 MPa @Strain 0.800 %, Temperature -20.0 °C |
2821 psi @Strain 0.800 %, Temperature -4.00 °F |
ISO 11403-1 -2 | |
| 20.17 MPa @Strain 30.0 %, Temperature 90.0 °C |
2925 psi @Strain 30.0 %, Temperature 194 °F |
ISO 11403-1 -2 | |
| 25.27 MPa @Strain 2.40 %, Temperature 40.0 °C |
3665 psi @Strain 2.40 %, Temperature 104 °F |
ISO 11403-1 -2 | |
| 26.91 MPa @Strain 1.40 %, Temperature 23.0 °C |
3903 psi @Strain 1.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
| 28.12 MPa @Strain 3.60 %, Temperature 40.0 °C |
4078 psi @Strain 3.60 %, Temperature 104 °F |
ISO 11403-1 -2 | |
| 30.15 MPa @Strain 6.00 %, Temperature 40.0 °C |
4373 psi @Strain 6.00 %, Temperature 104 °F |
ISO 11403-1 -2 | |
| 33.86 MPa @Strain 1.60 %, Temperature 0.000 °C |
4911 psi @Strain 1.60 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
| 35.74 MPa @Strain 2.20 %, Temperature 23.0 °C |
5184 psi @Strain 2.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
| 39.39 MPa @Strain 3.00 %, Temperature 23.0 °C |
5713 psi @Strain 3.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
| 43.96 MPa @Strain 2.00 %, Temperature -20.0 °C |
6376 psi @Strain 2.00 %, Temperature -4.00 °F |
ISO 11403-1 -2 | |
| 46.2 MPa @Strain 2.60 %, Temperature 0.000 °C |
6700 psi @Strain 2.60 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
| 51.41 MPa @Strain 3.80 %, Temperature 0.000 °C |
7456 psi @Strain 3.80 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
| 55.38 MPa @Strain 2.90 %, Temperature -20.0 °C |
8032 psi @Strain 2.90 %, Temperature -4.00 °F |
ISO 11403-1 -2 | |
| 61.78 MPa @Strain 4.00 %, Temperature -20.0 °C |
8960 psi @Strain 4.00 %, Temperature -4.00 °F |
ISO 11403-1 -2 | |
| Tensile Strength, Yield | 40.0 MPa | 5800 psi | ISO 527-1/-2 |
| Elongation at Break | 45 % | 45 % | Nominal; ISO 527-1/-2 |
| Elongation at Yield | 9.0 % | 9.0 % | ISO 527-1/-2 |
| Tensile Modulus | 2.20 GPa | 319 ksi | ISO 527-1/-2 |
| Flexural Modulus | 2.10 GPa | 305 ksi | ISO 178 |
| Secant Modulus | 0.06492 GPa @Strain 50.0 %, Temperature 40.0 °C |
9.416 ksi @Strain 50.0 %, Temperature 104 °F |
ISO 11403-1 -2 |
| 0.582 GPa @Strain 7.00 %, Temperature 23.0 °C |
84.4 ksi @Strain 7.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
| 0.71525 GPa @Strain 4.00 %, Temperature 40.0 °C |
103.74 ksi @Strain 4.00 %, Temperature 104 °F |
ISO 11403-1 -2 | |
| 1.05 GPa @Strain 2.40 %, Temperature 40.0 °C |
153 ksi @Strain 2.40 %, Temperature 104 °F |
ISO 11403-1 -2 | |
| 1.12 GPa @Strain 3.60 %, Temperature 23.0 °C |
162 ksi @Strain 3.60 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
| 1.2093 GPa @Strain 4.30 %, Temperature 0.000 °C |
175.40 ksi @Strain 4.30 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
| 1.2776 GPa @Strain 5.00 %, Temperature -20.0 °C |
185.30 ksi @Strain 5.00 %, Temperature -4.00 °F |
ISO 11403-1 -2 | |
| 1.448 GPa @Strain 1.00 %, Temperature 40.0 °C |
210.0 ksi @Strain 1.00 %, Temperature 104 °F |
ISO 11403-1 -2 | |
| 1.55 GPa @Strain 2.40 %, Temperature 23.0 °C |
224 ksi @Strain 2.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
| 1.63 GPa @Strain 3.00 %, Temperature 0.000 °C |
236 ksi @Strain 3.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
| 1.78 GPa @Strain 3.30 %, Temperature -20.0 °C |
258 ksi @Strain 3.30 %, Temperature -4.00 °F |
ISO 11403-1 -2 | |
| 1.92 GPa @Strain 1.40 %, Temperature 23.0 °C |
279 ksi @Strain 1.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
| 2.03 GPa @Strain 0.800 %, Temperature 23.0 °C |
295 ksi @Strain 0.800 %, Temperature 73.4 °F |
ISO 11403-1 -2 | |
| 2.12 GPa @Strain 1.60 %, Temperature 0.000 °C |
307 ksi @Strain 1.60 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
| 2.198 GPa @Strain 2.00 %, Temperature -20.0 °C |
318.8 ksi @Strain 2.00 %, Temperature -4.00 °F |
ISO 11403-1 -2 | |
| 2.305 GPa @Strain 0.800 %, Temperature 0.000 °C |
334.3 ksi @Strain 0.800 %, Temperature 32.0 °F |
ISO 11403-1 -2 | |
| 2.43 GPa @Strain 0.800 %, Temperature -20.0 °C |
353 ksi @Strain 0.800 %, Temperature -4.00 °F |
ISO 11403-1 -2 | |
| Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | ISO 180/1A |
| 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A | |
| 10.0 kJ/m² @Temperature -40.0 °C |
4.76 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB | NB | ISO 180/1U |
| 220 kJ/m² @Temperature -30.0 °C |
105 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U | |
| 220 kJ/m² @Temperature -40.0 °C |
105 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1U | |
| Charpy Impact Unnotched | NB | NB | ISO 179/1eU |
| 35.0 J/cm² @Temperature -30.0 °C |
167 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU | |
| 35.0 J/cm² @Temperature -40.0 °C |
167 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/1eA |
| 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA | |
| 1.00 J/cm² @Temperature -40.0 °C |
4.76 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 190 µm/m-°C | 106 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 190 µm/m-°C | 106 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 225 °C | 437 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 125 °C | 257 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 55.0 °C | 131 °F | ISO 75-1/-2 |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
IEC 60695-11-10 |
| V-0 @Thickness 0.800 mm |
V-0 @Thickness 0.0315 in |
IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |