| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.12 g/cc | 0.0405 lb/in³ | |
| 1.32 g/cc | 0.0477 lb/in³ | DAM; ISO 1183 | |
| Water Absorption at Saturation | 0.83 % | 0.83 % | DAM; Immersion 24h; ASTM D570 |
| Viscosity Test | 165 cm³/g | 165 cm³/g | DAM; ISO 307 1157 1628 |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 95.0 MPa | 13800 psi | 50%RH; ISO 527-1/-2 |
| 142 MPa | 20600 psi | DAM; ISO 527-1/-2 | |
| Tensile Stress | 21.14 MPa @Strain 0.600 %, Temperature 90.0 °C |
3066 psi @Strain 0.600 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
| 24.19 MPa @Strain 0.680 %, Temperature 90.0 °C |
3508 psi @Strain 0.680 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 | |
| 27.72 MPa @Strain 0.630 %, Temperature 40.0 °C |
4020 psi @Strain 0.630 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 30.07 MPa @Strain 0.400 %, Temperature 40.0 °C |
4361 psi @Strain 0.400 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| 32.25 MPa @Strain 0.570 %, Temperature 23.0 °C |
4677 psi @Strain 0.570 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 | |
| 52.19 MPa @Strain 2.24 %, Temperature 90.0 °C |
7570 psi @Strain 2.24 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 | |
| 61.57 MPa @Strain 2.69 %, Temperature 90.0 °C |
8930 psi @Strain 2.69 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 | |
| 62.48 MPa @Strain 3.89 %, Temperature 90.0 °C |
9062 psi @Strain 3.89 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 | |
| 70.96 MPa @Strain 2.40 %, Temperature 40.0 °C |
10290 psi @Strain 2.40 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 73.93 MPa @Strain 4.63 %, Temperature 90.0 °C |
10720 psi @Strain 4.63 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 | |
| 82.81 MPa @Strain 2.13 %, Temperature 23.0 °C |
12010 psi @Strain 2.13 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 | |
| 85.05 MPa @Strain 4.18 %, Temperature 40.0 °C |
12340 psi @Strain 4.18 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 91.14 MPa @Strain 1.57 %, Temperature 40.0 °C |
13220 psi @Strain 1.57 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| 100.16 MPa @Strain 3.70 %, Temperature 23.0 °C |
14527 psi @Strain 3.70 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 | |
| 115.12 MPa @Strain 2.74 %, Temperature 40.0 °C |
16697 psi @Strain 2.74 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| Elongation at Break | 4.0 % | 4.0 % | DAM; ISO 527-1/-2 |
| 5.0 % | 5.0 % | 50%RH; ISO 527-1/-2 | |
| Tensile Modulus | 5.80 GPa | 841 ksi | 50%RH; ISO 527-1/-2 |
| 8.70 GPa | 1260 ksi | DAM; ISO 527-1/-2 | |
| Flexural Modulus | 5.20 GPa | 754 ksi | 50%RH; ISO 178 |
| 7.40 GPa | 1070 ksi | DAM; ISO 178 | |
| Secant Modulus | 1.81 GPa @Strain 4.77 %, Temperature 40.0 °C |
263 ksi @Strain 4.77 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
| 2.41 GPa @Strain 4.22 %, Temperature 23.0 °C |
350 ksi @Strain 4.22 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 | |
| 2.96 GPa @Strain 2.40 %, Temperature 40.0 °C |
429 ksi @Strain 2.40 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 3.72 GPa @Strain 3.17 %, Temperature 40.0 °C |
539 ksi @Strain 3.17 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| 3.89 GPa @Strain 2.13 %, Temperature 23.0 °C |
564 ksi @Strain 2.13 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 | |
| 4.40 GPa @Strain 0.630 %, Temperature 40.0 °C |
638 ksi @Strain 0.630 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 | |
| 5.66 GPa @Strain 0.570 %, Temperature 23.0 °C |
821 ksi @Strain 0.570 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 | |
| 5.8051 GPa @Strain 1.57 %, Temperature 40.0 °C |
841.97 ksi @Strain 1.57 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| 7.5175 GPa @Strain 0.400 %, Temperature 40.0 °C |
1090.3 ksi @Strain 0.400 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 | |
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 50%RH; ISO 180/1A |
| 21.0 kJ/m² | 9.99 ft-lb/in² | DAM; ISO 180/1A | |
| 10.0 kJ/m² @Temperature -40.0 °C |
4.76 ft-lb/in² @Temperature -40.0 °F |
50%RH; ISO 180/1A | |
| 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A | |
| 14.0 kJ/m² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A | |
| 15.0 kJ/m² @Temperature -40.0 °C |
7.14 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | 74.0 kJ/m² | 35.2 ft-lb/in² | DAM; ISO 180/1U |
| 80.0 kJ/m² | 38.1 ft-lb/in² | 50%RH; ISO 180/1U | |
| 75.0 kJ/m² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1U | |
| 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1U | |
| Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | 50%RH; ISO 179/1eU |
| 9.10 J/cm² | 43.3 ft-lb/in² | DAM; ISO 179/1eU | |
| 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU | |
| 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | DAM; ISO 179/1eA |
| 2.20 J/cm² | 10.5 ft-lb/in² | 50%RH; ISO 179/1eA | |
| 1.30 J/cm² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA | |
| 1.30 J/cm² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
50%RH; ISO 179/1eA | |
| 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
| 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | DAM; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 119 µm/m-°C | 66.1 µin/in-°F | DAM; ISO 11359-1/-2 |
| 95.0 µm/m-°C @Temperature -40.0 °C |
52.8 µin/in-°F @Temperature -40.0 °F |
ISO 11403-1 -2 | |
| 95.0 µm/m-°C @Temperature 23.0 °C |
52.8 µin/in-°F @Temperature 73.4 °F |
ISO 11403-1 -2 | |
| 95.0 µm/m-°C @Temperature 95.0 °C |
52.8 µin/in-°F @Temperature 203 °F |
ISO 11403-1 -2 | |
| Specific Heat Capacity | 2.20 J/g-°C | 0.526 BTU/lb-°F | |
| Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | of melt |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 600 V | 600 V | DAM; IEC 60112 |