| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled |
| Manufacturer | EMS-Grivory (EMS-CHEMIE) |
| Trade Name | Grivory® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | EMS-Grivory Grivory® BG-30 EC PA6-GF30.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
| Water Absorption | 7.0 % | 7.0 % | ISO 62 |
| Moisture Absorption | 2.00 % | 2.00 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 80.0 MPa | 11600 psi | conditioned; ISO 2039-1 |
| 170 MPa | 24700 psi | dry; ISO 2039-1 | |
| Tensile Strength at Break | 80.0 MPa | 11600 psi | conditioned; ISO 527-1/-2 |
| 100 MPa | 14500 psi | dry; ISO 527-1/-2 | |
| Tensile Strength, Yield | 80.0 MPa | 11600 psi | conditioned; ISO 527-1/-2 |
| 115 MPa | 16700 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 6.0 % | 6.0 % | dry; ISO 527-1/-2 |
| 10 % | 10 % | conditioned; ISO 527-1/-2 | |
| Elongation at Yield | 3.0 % | 3.0 % | dry; ISO 527-1/-2 |
| 5.0 % | 5.0 % | conditioned; ISO 527-1/-2 | |
| Tensile Modulus | 5.00 GPa | 725 ksi | conditioned; ISO 527-1/-2 |
| 9.40 GPa | 1360 ksi | dry; ISO 527-1/-2 | |
| Charpy Impact Unnotched | 5.00 J/cm² | 23.8 ft-lb/in² | dry; ISO 179/1eU |
| 6.00 J/cm² | 28.6 ft-lb/in² | conditioned; ISO 179/1eU | |
| 3.00 J/cm² @Temperature 30.0 °C |
14.3 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 3.00 J/cm² @Temperature 30.0 °C |
14.3 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | dry; ISO 179/1eA |
| 1.00 J/cm² | 4.76 ft-lb/in² | conditioned; ISO 179/1eA | |
| 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
| Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
| 160 °C | 320 °F | short term; EMS | |
| Deflection Temperature at 1.8 MPa (264 psi) | 205 °C | 401 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB | HB | IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2500 ohm-cm | 2500 ohm-cm | dry; IEC 60093 |
| Surface Resistance | 1e+05 | 1e+05 | IEC 60093 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Form | Granules | |
| Processing | Injection Molding | |
| Special Characteristics | Anti-static |