| Category | Polymer , Film , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Film Grade |
| Manufacturer | Lanxess |
| Trade Name | Durethan® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Lanxess Durethan® B 40 F 000000 Nylon 6, Film Grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
| Water Absorption | 10 % | 10 % | Test Sim. to ISO 62 |
| Moisture Absorption at Equilibrium | 3.0 % | 3.0 % | 23°C/50% R.H.; Test Sim. to ISO 62 |
| Viscosity Test | 225 cm³/g | 225 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
| Melt Flow | 3 g/10 min @Load 2.16 kg, Temperature 235 °C |
3 g/10 min @Load 4.76 lb, Temperature 455 °F |
Estimated using room temperature density; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | Conditioned; ISO 527-1/-2 |
| 75.0 MPa | 10900 psi | ISO 527-1/-2 | |
| Elongation at Break | 20 % | 20 % | Nominal; ISO 527-1/-2 |
| >= 50 % | >= 50 % | Nominal, Conditioned; ISO 527-1/-2 | |
| Elongation at Yield | 4.0 % | 4.0 % | ISO 527-1/-2 |
| 25 % | 25 % | Conditioned; ISO 527-1/-2 | |
| Tensile Modulus | 0.800 GPa | 116 ksi | Conditioned; ISO 527-1/-2 |
| 2.80 GPa | 406 ksi | ISO 527-1/-2 | |
| Charpy Impact Unnotched | NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
Conditioned; ISO 179/1eU | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eU | |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
Conditioned; ISO 179/1eU | |
| Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| <= 0.500 J/cm² @Temperature -30.0 °C |
<= 2.38 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eA | |
| 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA | |
| 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75-1/-2 |
| Deflection Temperature at 8.0 MPa | 40.0 °C | 104 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB | HB | IEC 60695-11-10 |
| HB | HB | IEC 60695-11-10 | |
| Oxygen Index | 24 % | 24 % | ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | Conditioned; IEC 60093 |
| 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 | |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Dielectric Constant | 3.5 @Frequency 1.00e+6 Hz |
3.5 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.9 @Frequency 100 Hz |
3.9 @Frequency 100 Hz |
IEC 60250 | |
| 4.0 @Frequency 1.00e+6 Hz |
4.0 @Frequency 1.00e+6 Hz |
Conditioned; IEC 60250 | |
| 18 @Frequency 100 Hz |
18 @Frequency 100 Hz |
Conditioned; IEC 60250 | |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243-1 |
| 35.0 kV/mm | 889 kV/in | Conditioned; IEC 60243-1 | |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Form | Pellets | |
| ISO Shortname | ISO 1874: PA 6, FN,22,030 | |
| Processing | Film extrusion | |
| Region | Asia Pacific | |
| Europe | ||
| Near East/Africa | ||
| North America | ||
| South and Central America |