| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded |
| Manufacturer | Polymer Resources, LTD |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
| Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 70 | 70 | ASTM D785 |
| Hardness, Rockwell R | 118 | 118 | ASTM D785 |
| Tensile Strength at Break | 68.9 MPa | 10000 psi | ASTM D638 |
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
| Elongation at Break | 140 % | 140 % | ASTM D638 |
| Elongation at Yield | 6.5 % | 6.5 % | ASTM D638 |
| Flexural Strength | 95.8 MPa | 13900 psi | ASTM D790 |
| Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
| Izod Impact, Notched | 8.01 J/cm @Temperature 22.8 °C |
15.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 135 °C | 275 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
| Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
| UL RTI, Electrical | 80.0 °C @Thickness 0.749 mm |
176 °F @Thickness 0.0295 in |
UL 746 |
| 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
UL 746 | |
| 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746 | |
| UL RTI, Mechanical with Impact | 80.0 °C @Thickness 0.749 mm |
176 °F @Thickness 0.0295 in |
UL 746 |
| 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
UL 746 | |
| 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746 | |
| UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.749 mm |
176 °F @Thickness 0.0295 in |
UL 746 |
| 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
UL 746 | |
| 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
UL 746 | |
| Flammability, UL94 | V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
|
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 1.0 % | 1.0 % | ASTM D1003 |
| UV Transmittance | 88 % | 88 % | ASTM D1003 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
| Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746 |
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
| 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL 746 | |
| High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL 746 |
| >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
UL 746 | |
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
| Melt Temperature | 288 - 316 °C | 550 - 600 °F | |
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Outdoor Suitability | f1 | |
| Vent | 0.0005 |