| Category | Polymer , Thermoplastic , Polyetherimide (PEI) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | ULTEM |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics ULTEM 2210 PEI (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.550 % | 0.550 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 1.0 % | 1.0 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | on Tensile Bar; SABIC Method |
| Melt Index of Compound | 10 g/10 min @Load 5.00 kg, Temperature 360 °C |
10 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, H358/30 | 150 MPa | 21800 psi | ISO 2039-1 |
| Tensile Strength at Break | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
| Elongation at Break | 2.0 % | 2.0 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
| Flexural Strength | 210 MPa | 30500 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 6.50 GPa | 943 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
| 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U | |
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
| 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU | |
| Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | ISO 179/2C |
| Taber Abrasion, mg/1000 Cycles | 17 | 17 | CS-17, 1 kg; SABIC Method |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 25.0 µm/m-°C @Temperature 23.0 - 150 °C |
13.9 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
| CTE, linear, Transverse to Flow | 60.0 µm/m-°C @Temperature 23.0 - 150 °C |
33.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
| Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 205 °C | 401 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| Vicat Softening Point | 212 °C | 414 °F | Rate B/50; ISO 306 |
| 218 °C | 424 °F | Rate B/120; ISO 306 | |
| 223 °C | 433 °F | Rate A/50; ISO 306 | |
| Glass Transition Temp, Tg | 217 °C | 423 °F | |
| UL RTI, Electrical | 170 °C | 338 °F | UL 746B |
| UL RTI, Mechanical with Impact | 170 °C | 338 °F | UL 746B |
| UL RTI, Mechanical without Impact | 170 °C | 338 °F | UL 746B |
| Flammability, UL94 | V-0 @Thickness 0.410 mm |
V-0 @Thickness 0.0161 in |
UL 94 |
| 5VA @Thickness 1.90 mm |
5VA @Thickness 0.0748 in |
UL 94 | |
| Oxygen Index | 46 % | 46 % | ISO 4589 |
| Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ROA; IEC 60093 |
| Dielectric Constant | 3.0 @Frequency 1.00e+6 Hz |
3.0 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.1 @Frequency 50.0 - 60.0 Hz |
3.1 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
| Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
| 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 | |
| 34.0 kV/mm @Thickness 0.800 mm |
864 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 | |
| Dissipation Factor | 0.00080 @Frequency 50.0 - 60.0 Hz |
0.00080 @Frequency 50.0 - 60.0 Hz |
IEC 60250 |
| 0.0025 @Frequency 1.00e+6 Hz |
0.0025 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| 0.0049 @Frequency 2.45e+9 Hz |
0.0049 @Frequency 2.45e+9 Hz |
IEC 60250 | |
| Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
| 150 V | 150 V | IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |