| Category | Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler |
| Manufacturer | Solvay Specialty Polymers |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.68 g/cc | 0.0607 lb/in³ | ASTM D792 |
| Filler Content | 40 % | 40 % | Glass Fiber |
| Water Absorption | 0.020 % @Time 86400 sec |
0.020 % @Time 24.0 hour |
ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0020 cm/cm @Thickness 3.18 mm |
0.0020 in/in @Thickness 0.125 in |
|
| Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Thickness 3.20 mm |
0.0050 in/in @Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 104 | 104 | ASTM D785 |
| Hardness, Rockwell R | 122 | 122 | ASTM D785 |
| Tensile Strength | 179 MPa | 26000 psi | ASTM D638 |
| Tensile Stress | 170 MPa | 24700 psi | ISO 527-2 |
| Elongation at Break | 1.2 % | 1.2 % | ASTM D638 |
| 1.3 % | 1.3 % | ISO 527-2 | |
| Flexural Strength | 228 MPa | 33100 psi | ASTM D790 |
| 245 MPa | 35500 psi | ISO 178 | |
| Flexural Modulus | 14.0 GPa | 2030 ksi | ISO 178 |
| 14.5 GPa | 2100 ksi | ASTM D790 | |
| Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
| Poissons Ratio | 0.43 | 0.43 | ASTM E132 |
| Izod Impact, Notched | 0.910 J/cm @Thickness 3.18 mm |
1.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Izod Impact, Unnotched | 4.50 J/cm @Thickness 3.18 mm |
8.43 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Izod Impact, Notched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | Notch A; ISO 180 |
| Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 100 - 200 °C |
8.33 µin/in-°F @Temperature 212 - 392 °F |
2 |
| 15.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
8.33 µin/in-°F @Temperature -58.0 - 122 °F |
2 | |
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
22.2 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
| 80.0 µm/m-°C @Temperature 100 - 200 °C |
44.4 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 | |
| Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
| Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | Unannealed; ASTM D648 |
| Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
|
| 5VA @Thickness 1.60 mm |
5VA @Thickness 0.0630 in |
||
| Oxygen Index | 50 % | 50 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Insulation Resistance | 1.00e+12 ohm @Temperature 90.0 °C |
1.00e+12 ohm @Temperature 194 °F |
IEC 60167 |
| Dielectric Constant | 3.9 @Frequency 1000 Hz |
3.9 @Frequency 1000 Hz |
ASTM D150 |
| 3.9 @Frequency 1.00e+6 Hz |
3.9 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D149 |
| Dissipation Factor | 0.0020 @Frequency 1000 Hz |
0.0020 @Frequency 1000 Hz |
ASTM D150 |
| 0.0020 @Frequency 1.00e+6 Hz |
0.0020 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| Arc Resistance | 125 sec | 125 sec | ASTM D495 |
| Comparative Tracking Index | 150 V | 150 V | UL 746 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Availability | Asia Pacific | |
| Europe | ||
| Latin America | ||
| North America | ||
| Color | Natural | |
| Form | Pellets | |
| Processing Technique | Injection Molding | |
| RoHS Compliance | RoHS Compliant |